The invention discloses a method for separating enriched
nickel and
cobalt from a
laterite nickel ore lixivium, which comprises the following steps: after
solid and liquid separation between the
laterite nickel ore lixivium and ore
slag is implemented, a vulcanizing agent is added into the lixivium, the
solid and the liquid are separated after reaction
precipitation, and precipitated
solid is washed by a new lixivium, thus obtaining
sulfide precipitate; after the
sulfide precipitate is pulpified, sulphuric acid and solution of
nitric acid and mixed acid are added so as to implement oxidizing leaching; the
goethite method is adopted for removing iron from a superior pickle liquor; a
sodium thiosulfate solution is added so as to implement
copper removing; a filtering liquor that is the enriched nickel and
cobalt solution is obtained. Compared with the prior art, the method for separating enriched nickel and
cobalt from the
laterite nickel ore lixivium is implemented at normal temperature and normal pressure, does not need a high-pressure caldron, has less device investment, low running cost, simple technical path, short process and controllable production scale; the vulcanizing agent and acids that are used in the technique can be recycled to the utmost extent and do not have emissions and environment
pollution; the extraction yield of nickel and cobalt can achieve over 95 percent, and the method for separating enriched nickel and cobalt from the laterite nickel ore lixivium has low production cost and easy industrialization.