The invention provides a low-
chromium high-absorption tanning method. The low-
chromium high-absorption tanning method comprises the following steps: step 1, weighing and metering: weighing
raw material leather as a material metering basis for subsequent procedures of soaking, liming, washing, pre-deliming, deliming,
softening,
pickling, tanning and the like; step 2, soaking: adding water which submerges the raw leather into the raw leather; step 3, liming; step 4, washing with water; step 5, pre-deliming; step 6, deliming and
softening: adding 0.5-1 time of 30 DEG C water, adding 0.8% of a deliming agent and 0.2% of a
degreasing agent, adding
sulfuric acid to adjust the pH value to 3.5, and adding 0.5% of
softening compound
enzyme and 0.5% of an auxiliary agent; step 7,
pickling and tanning: adding 1.5% of a
pickling aid, rotating for 60-90 minutes, adding 2-3% of a chrome tanning agent, rotating for 60-90 minutes, adding 1-1.5% of a tanning aid, and rotating for 60-90 minutes; the method has the characteristics of reducing environmental
pollution and ensuring that the quality index of a finished product is not reduced.