The invention discloses a method for producing a stair
tread. The method comprises the following steps that a, a board made of
beech materials is
cut into a panel for making the stair
tread, and a product A is obtained; b, planning of the product A is carried out, and a product B is obtained; c, two aluminum plates are placed on the front and back two sides of the product B to achieve tight clamping, and a product C is obtained; d, the product C is placed into a
kiln to be carbonized, the
carbonization temperature is 180-210 DEG C, the
carbonization time is 1-2 h, ultrasonic treatment of the product C is carried out while
carbonization is carried out, the frequency of ultrasonic
waves is 40-45 KHz, and a product D is obtained; e, the aluminum plates on the product D are removed, then the product D is placed into a resurgence chamber, the
moisture content of the product D rises to 7%-9%, and a product E is obtained; f, the product E is subjected to paint treatment, and a product F is obtained; g, the product F is covered with tea to be then put into the
kiln for heat preservation, and a product G is obtained; h,
phenol is used for
fumigation of the product G, and a product H is obtained; and i, ethyl
alcohol is used for scrubbing the surface of the product H, the surface of the product H is made clean and tidy, and a finished product is obtained. The stair
tread manufactured through the method has the advantages of being not prone to generating
noise and being small in paint
odor.