The invention discloses an anti-oxidizing rubber material including, by weight, 9-11 parts of polyethylene glycol terephthalate, 2-5 parts of trioctyl citrate, 2-4 parts of a softener, 2-4 parts of plant polyphenol, 22-25 parts of polyacrylonitrile, 1-2 parts of sodium diacetate, 12-15 parts of graphite, 3-4 parts of micro beads of fly ash, 0.5-1 part of lauryl sodium sulfate, 40-60 parts of liquid nitrile butadiene rubber, 0.5-1 part of methylacrylic acid, 50-60 parts of nitrile butadiene rubber, 20-25 parts of styrene butadiene rubber, 5-8 parts of nano silicon sol, 3-4 parts of tetramethyl thiuram disulfide, 2-3 parts of diethylene glycol, 6-8 parts of VAE emulsion, 14-16 parts of a filling agent, 7-10 parts of magnesium hydroxide, and 0.2-0.4 parts of calcium propanoate. The anti-oxidizing rubber material has excellent water proof performance, is acid-resistant, oil-resistant and flame-retarding and satisfies demands in production well.