The invention discloses dealcoholized
room temperature vulcanized
silicone rubber and a preparation method thereof. The vulcanized
silicone rubber comprises the following components of: alpha,
omega-dihydroxypolydimethylsiloxane, dimethicone, reinforcing filler, a cocatalyst, a first cross-linking agent, a
silane coupling agent, a second cross-linking agent and a catalyst. The preparation method thereof comprises the steps of: adding the alpha,
omega-dihydroxypolydimethylsiloxane, dimethicone and reinforcing filler into a vacuum stirring kettle, performing stirring for
dehydration at 130-170 DEGC and (-0.09)-(-0.1) MPa for 2-4 hours, and performing cooling to obtain base rubber; and adding the cocatalyst and first cross-linking agent sequentially into the base rubber, performing
vacuum pumping and even stirring, then adding the
silane coupling agent, second cross-linking agent and catalyst sequentially, performing
vacuum pumping to (-0.09)-(-0.1) MPa, and performing stirring to obtain the dealcoholized
room temperature vulcanized
silicone rubber. During preparation of the vulcanized
silicone rubber by using the preparation method, no
viscosity peaks are generated, and the problem ofhigh
energy consumption caused by rapid thickening of rubber
viscosity is solved.