Patents
Literature
Hiro is an intelligent assistant for R&D personnel, combined with Patent DNA, to facilitate innovative research.
Hiro

34results about How to "Avoid poisonous" patented technology

Method for purifying panaxoside compound-K by applying macroporous resin

The invention relates to a method for separating and purifying a panaxoside compound-K from microorganism zymocyte by applying macroporous resin for preparing a raw medicine. The purifying yield reaches more than 72 percent, and the content of the panaxoside compound-K in a product is more than 96 percent. The method mainly comprises the following steps of: adding ethanol into zymocyte for extracting and concentrating; decoloring by active carbon and filtering; after adding water into filter liquor for diluting, leading the filter liquor to pass through a macroporous resin chromatographic column; washing by a low-concentration organic solvent aqueous solution for removing pigment and high-polarity saponin; eluting by a high-concentration organic solvent aqueous solution to obtain a panaxoside compound-K component; and finally crystallizing to obtain the panaxoside compound-K raw medicine with the content of more than 96 percent. The invention can provide a great amount of qualified raw medicine samples for the pharmaceutical development of the panaxoside compound-K.
Owner:ZHEJIANG HISUN PHARMA CO LTD

Chemiluminescence immune analysis determination reagent kit for detecting Toxoplasma Gondi IgM antibody

The invention discloses a toxoplasma gondii IgM antibody detection kit combined with the FITC-anti-FITC indirect coating technology and the chemiluminescent immunoassay technology, and a preparation method thereof. The kit of the invention is composed of a negative control, a positive control, solid-phase vectors for anti-FITC antibodies, anti-human Mu-chain monoclonal antibodies of FITC markers, toxoplasma gondii antigens which are marked by horse radish peroxidase, chemiluminescent substrates and concentrated washing solutions. The kit of the invention can be used as the aided detection index for prenatal prepotency diagnosis, and has vital significances for improving the birth population quality and doing the family planning and the prepotency well.
Owner:CHEMCLIN DIAGNOSTICS CO LTD

Neutral blockage removing agent composition used for oil recovery formation in oilfield and preparation method thereof

The invention relates to a neutral blockage removing agent composition used for an oil recovery formation in an oilfield. The neutral blockage removing agent composition is prepared from the following raw materials in parts by weight: 10-14 parts of polyepoxysuccinic acid amine, 35-40 parts of diethylenetriaminepentaacetic acid amine, 33-37 parts of hydroxyl succinic acid amine, 20-25 parts of polyacrylamide, 7-10 parts of sodium polyaspartate, 10-14 parts of sodium gluconate, 10-15 parts of activated clay, 20-25 parts of potassium peroxodisulfate, 9-11 parts of hydroxyl butanedioic acid amine, 4-7 parts of sodium salicylate, 5-9 parts of hexamethylene tetramine, 0.2-0.3 part of vanadium pentoxide, 2-5 parts of starch, 5-8 parts of alpha-sulphonated fatty acid methyl ester and derivative thereof (MES) and 0.1-0.3 part ofdiethyl ethanolamine. The neutral blockage removing agent composition is used for the blockage removal of an oil pumping well and a screw pump well in the oilfield, can effectively solve the problems of cleaning blockage removal of the oil pumping well and the screw pump well in the oilfield and the corrosion of oil recovery equipment, has high blockage removing speed, is neutral and is free of corrosion; waste liquid for blockage removal can be degraded and does not need to be discharged onto the ground to be subjected to sewage treatment, no corrosion, dead angle, precipitation or secondary well blockage are generated, and more safety and more reliability are realized as compared with traditional pickling blockage removing, biological blockage removing and solvent blockage removing.
Owner:兰州熙瑞化工科技有限公司

Double-strand oligonucleotide-epsilon-polylysine compound with immune regulation function and preparation and use method of double-strand oligonucleotide-epsilon-polylysine compound

The invention provides a double-strand oligonucleotide-epsilon-polylysine compound with an immune regulation function and a preparation and use method of the double-strand oligonucleotide-epsilon-polylysine compound and also provides immunogen composition with functions of triggering immunoenhancement reaction and changing the immunoreaction type and a preparation and use method of the immunogen composition. The immunogen composition comprises the double-strand oligonucleotide-epsilon-polylysine compound and an antigen. The compound contains a compound formed through composition of double-stranded polynucleotide, a cation epsilon-polylysine and metal cations. The compound has the pharmacological activity of immunoregulation. The preparation process of the compound is simple. The compound has good water solubility and a bio-enzyme degradation resisting function. The immunogen composition can trigger the immunoenhancement reaction and change the immunoreaction type.
Owner:辽科生物(沈阳)有限公司

Ginkgo juice beverage and preparation method thereof

The invention discloses a ginkgo juice beverage and a preparation method thereof. The ginkgo juice beverage comprises the following components in percentage by weight: 10-30% of ginkgo normal juice, 2.5-8% of saccharose, 0.1-0.35% of citric acid and the balance of purified water. The beverage is prepared by the following steps of: weighing the ginkgo normal juice according to the formula and slowly pouring into an allocating tank; then, respectively dissolving saccharose and citric acid by using purified water and adding purified water to 100%; heating to 50 DEG C, and adequately and uniformly stirring; filtering by a frame filter and homogenizing the filtrate by a Fluko efficient dispersing emulsifying machine for 8-12 minutes at a high speed so as to further uniformly refine the feed liquid; filling the homogenized beverage in a high-temperature resisting glass bottle, sealing, and sterilizing in a sterilizing pot for 15 minutes at 120-121 DEG C, taking out and naturally cooling; and inspecting and packaging to obtain the finished product. The product disclosed by the invention is clear in liquid, is rich and pleasant, fresh in taste and agreeable in sweet and sour tastes, and has special fragrance of ginkgo and good market prospect.
Owner:徐州绿之野生物食品有限公司

Preparation method of Abemaciclib intermediate

The invention belongs to the field of medicine and chemical industry, and concretely relates to a preparation method of an Abemaciclib intermediate. Nitro and carbonyl of 5-(4-ethyl piperazine-1-carbonyl)-2-nitropyridine are reduced successively, and the Abemaciclib intermediate 5-(4-ethyl-piperazin-1-yl)methyl)pyridin-2-amine is obtained; the raw materials and reagents are easy to obtain, reaction conditions are mild, usage of reagents with toxicity or irritation or strong corrosivity is avoided, the method is green and environmentally friendly, and the preparation is simple and easy to operate; the product has high yield and high purity, and is especially suitable for industrial production.
Owner:CHIA TAI TIANQING PHARMA GRP CO LTD

Preparation process of epoxy compound

InactiveCN103896885ASafety scale-up productionAvoid poisonousOrganic chemistryEpoxyCombinatorial chemistry
The invention discloses a preparation process of an epoxy compound. The preparation process comprises the steps of enabling alkene to react with a halogenating agent in water or a mixed solvent, and performing alkali treatment to obtain the epoxy compound. The epoxy compound can be prepared through a one-pot method by preparing halogenated alcohol through reaction between a halogenating reagent containing NBS and alkene and then enabling the halogenated alcohol to react with alkali without the separation of intermediates. The preparation process disclosed by the invention avoids highly-toxic and high-explosive reagents applied to a conventional process method, so that the production of the epoxy compound can be safely amplified.
Owner:CHEN STONE GUANGZHOU CO LTD

Tire tread and preparation method thereof

The invention relates to tire tread which comprises 1-60 parts of solution polymerized styrene-butadiene rubber, 1-40 parts of natural rubber, 1.5 parts of environment-friendly promoter, 10-100 parts of high-dispersion white carbon black, 1-8 parts of silane coupling agent, 10-50 parts of carbon black and 1-20 parts of petroleum-series aromatic hydrocarbon oil. Preferably, the environment-friendly promoter is a compound of zinc dialkyl dithiophsophate and a carrier. The invention further provides a preparation method of the tire tread. The preparation process is divided into three adding and mixing stages, and the environment-friendly promoter is added at the productive stage. The tire tread and the preparation method have the advantages that combined use of the solution polymerized styrene-butadiene rubber, the natural rubber, the high-dispersion white carbon black, the silane coupling agent and the environment-friendly promoter is considered important for promoting scorching time, improving modulus and wear performance and lowering rolling resistance. By using the environment-friendly promoter, toxic, allergic and carcinogenic risks in the operation process can be avoided.
Owner:SHANDONG LINGLONG TIRE

Synthetic method for preparing steroid compounds from 3,17-diketone steroids

InactiveCN103450305AAvoid poisonousAvoid the disadvantages of being volatileSteroidsWittig reactionDrug
The invention discloses a synthetic method of steroid type drugs and intermediates, in particular relates to a synthetic method for preparing 17-hydroxy-20-ketone steroid compounds from 3,17-diketone steroids, and belongs to the field of synthesis of drugs. The method takes 3,17-diketone steroids as raw materials and adopts a conventional, environment-friendly, low-toxicity reagent, and the steroid type drugs such as cortisone, hydrocortisone, metacortandracin, or hydroprednisone, or intermediates 17alpha-hydroxy-20-ketone compounds are prepared simply and conveniently at high yield by selective protection of C3 or (and) C11-ketone group, Wittig reaction of C17, selective oxidization of 17(20)-position double bonds and halogenating replacement. The aftertreatment is simple, few three wastes are generated, the reaction selectivity is good, the yield is high, and byproducts anti-pregnancy steroidal drugs and steroidal compounds can be obtained. The raw materials are easy to get, the cost is low and the synthetic process is simple; the synthetic method is suitable for industrial production.
Owner:ZHENGZHOU UNIV

Adhesive hydrogel and preparation method thereof

ActiveCN110790949AViscoelastic regulationSoft texturePolymer sciencePhoto irradiation
The invention provides adhesive hydrogel and a preparation method thereof, and relates to the field of polymer materials. The method comprises the following steps: (1) mixing a cationic monomer, a photoinitiator, an anionic component and water to obtain a precursor solution; (2) defoaming the precursor solution; (3) irradiating the precursor solution obtained in the step (2) with ultraviolet lightto initiate cationic monomer polymerization, and reacting the generated cationic monomer polymer with the anionic component to form the adhesive hydrogel; wherein in the step (1), the anionic component comprises glycosaminoglycan and derivatives thereof. The adhesive hydrogel disclosed by the invention is soft in texture, can be used for bonding various surfaces, is high in adhesion strength andhas self-healing performance, and the practicability of the gel is improved.
Owner:TIANJIN POLYTECHNIC UNIV

One-step synthesis method of polyethyleneimine

ActiveCN113527674AOmission of processingOmit the regeneration processAlkanePtru catalyst
The invention relates to a one-step synthesis method of polyethyleneimine. The method comprises the following steps: (1) synthesizing monomer ethyleneimine, reacting ethanolamine with concentrated sulfuric acid or hydrogen chloride, and treating with strong base to obtain monomer ethyleneimine and an inorganic salt byproduct; and (2) synthesizing polyethyleneimine, namely directly polymerizing the monomer ethyleneimine obtained in the step (1) under the conditions of an acid catalyst and a polyhaloalkane catalyst without separation treatment to generate polyethyleneimine. According to the one-step synthesis method, on one hand, the use and storage risk and harm caused by high reactivity, corrosivity, toxicity, flammability and explosiveness of the ethyleneimine are avoided; on the other hand, special treatment for removing residual ethyleneimine in the monomer separation process is also avoided. According to the method disclosed by the invention, an intermediate separation step is not needed, so that the possible risks of poisoning, combustion and explosion to operators are greatly reduced, and the pressure of environmental protection is also greatly reduced.
Owner:上海氟聚化学产品股份有限公司

Potassium iodate preparation method

InactiveCN108083232AProduct particles are uniformAvoid poisonousIodine oxygen compoundsThermal insulationChemistry
The invention relates to a potassium iodate preparation method, which comprises: (1) dissolving potassium iodide containing a small amount of hydroiodic acid in water to prepare a potassium iodide aqueous solution with a mass concentration of 30-40%; (2) at a room temperature, respectively introducing the potassium iodide aqueous solution and 28-30 wt% hydrogen peroxide into the glass module of amicrochannel reactor by a feeding pump according to a mass ratio of (1.0-1.4):1, and carrying out a mixing reaction to obtain a first reaction liquid; (3) introducing the first reaction liquid and 28-30 wt% of hydrogen peroxide into the microchannel reactor according to a mass ratio of (39-48):1, and carrying out a reaction to obtain a second reaction liquid; and (4) collecting the second reactionliquid, heating to a temperature of 75-85 DEG C, filtering, carrying out cooling crystallization, carrying out thermal insulation at a temperature of 39-41 DEG C, adding crystal seed, crystallizing,cooling to a temperature of 4-6 DEG C, and carrying out thermal insulation to obtain the potassium iodate product. According to the present invention, the high-quality potassium iodate is quantitatively prepared by using the safe and environmentally-friendly reagents so as to achieve the high utilization rate of iodine.
Owner:SINOPHARM CHEM REAGENT

Preparation method of imatinib

The invention discloses a preparation method of imatinib, wherein the needed component imatinib is finally generated through conversion of an intermediate. According to the preparation method of the imatinib disclosed by the invention, the synthetic steps are fewer, the raw materials adopted are cheap and easy to obtain, the environment is less polluted, and the yield is high, so that the preparation method of the imatinib is appropriate for industrial production.
Owner:湖南欧亚药业有限公司

Magnesium alloy surface chemical nickel-plating combination solution for pre-electroplated zinc-nickel alloy

The invention discloses a magnesium alloy surface chemical nickel-plating combination solution for a pre-electroplated zinc-nickel alloy. The combination solution is characterized by comprising an electroplated zinc-nickel plating solution and a chemical nickel-plating solution. The components of the electroplated zinc-nickel plating solution and the chemical nickel-plating solution are adjusted, and toxic and high-pollution components are not adopted, so that the plating process is environment-friendly and safe, and the prepared coating is high in corrosion resistance, beautiful in appearance and high in binding force of a substrate and the coating.
Owner:无锡市锡山区鹅湖镇荡口青荡金属制品厂

Secondary galvanizing pretreatment process for electroplating nickel on surface of magnesium alloy

The invention discloses a secondary galvanizing pretreatment process for electroplating nickel on the surface of magnesium alloy. The secondary galvanizing pretreatment process comprises two steps of: zinc galvanizing and zinc electroplating. The pretreatment process disclosed by the invention has the advantages that pretreatment for nickel electroplating is carried out by adopting a secondary zinc galvanizing and coating process of zinc immersion and zinc electroplating, and by adjustment of the components for zinc immersion and zinc electroplating solution, components with toxicity and high pollution are not adopted, so that the plating process is environmentally friendly and safe and provides good basic plating layer for the following nickel plating.
Owner:无锡市锡山区鹅湖镇荡口青荡金属制品厂

Composition solution for electric nickel-plating on surface of magnesium alloy

The invention discloses a composition solution for electric nickel-plating on the surface of a magnesium alloy. The composition solution comprises a zinc immersion liquid, an electric zinc plating liquid and a nickel-electroplating liquid. By adjusting the components of the zinc immersion liquid, the zinc electroplating liquid and the nickel electroplating liquid, a plating process is environmental friendly and safe, and a prepared plated layer is high in corrosion resistance, attractive in appearance and high in binding force with a substrate.
Owner:无锡市锡山区鹅湖镇荡口青荡金属制品厂

Secondary zinc plating pretreatment composite solution for electroplating nickel on magnesium alloy surface

The invention discloses a secondary zinc plating pretreatment composite solution for electroplating nickel on a magnesium alloy surface. The composite solution comprises a zinc immersion solution and a zinc electroplating solution, wherein the zinc immersion solution is composed of the following components: zinc sulfate with a concentration of 32-36 g / L, potassium pyrophosphate with a concentration of 200-210 g / L, sodium carbonate with a concentration of 8-10 g / L, potassium fluoride with a concentration of 3-5 g / L, ammonium bifluoride with a concentration of 2-3 g / L, and the balance being water; and the zinc electroplating solution is composed of the following components: ZnSO4.7H2O with a concentration of 32-36 g / L, KF with a concentration of 18-20 g / L, K4P2O7.3H2O with a concentration of 164-168 g / L, C6H17O7N3 with a concentration of 32-36 g / L, phytic acid with a concentration of 0.4-0.6 g / L, H2CSNH2 with a concentration of 4-6 g / L, and the balance being water.
Owner:无锡市锡山区鹅湖镇荡口青荡金属制品厂

Preparation of poly(2,5-diakoxy-1,4-benzene)

InactiveCN1583813AGood location regularityAvoid poisonousBenzeneMetal chloride
2,5-dialkyloxy-1,4-benzene is prepared by solid state oxidized coupling polymerization, which includes: selecting p-dialkyloxylbenzene as monomer with C1-18 in alkyloxyl and metal chloride as catalyst, mixing and abrasing at 5-65deg.C and reacting for 10-30 minutes to obtain the crude product, separating and purifying to get poly(2,5- dialkyloxyl-1,4-benzene). Because of no solvent in polymerization, it reduces environment pollution, lower production cost, short polymerization time of only 10-30 minutes to increase productivity, increasing polymerization yield up to 90%. The obtained product has good structure regional mapping orderliness. Between phenyl cycles there are chain connections of contraposition. The obtained polymer has a fluorescence emission peak value of 405 nanometers or so, belonging to blue fluorescence emission materials. The conjugate polymers can be used to make electroluminescence parts of apparatus, organic thin-film transistor and other photoelectric conversion parts of apparatus.
Owner:WUHAN UNIV

3D blowing membrane

The invention discloses 3D blowing membrane. The 3D blowing membrane comprises an annular membrane body, wherein the annular membrane body comprises a TPU membrane layer, an anti-corrosion layer is attached to the upper end of the TPU membrane layer, an anti-impact layer is attached to the upper end of the anti-corrosion layer, a high-tenacity layer is attached to the upper end of the anti-impactlayer, a high-elasticity layer is attached to the upper end of the high-tenacity layer, a low temperature resisting layer is attached to the upper end of the high-elasticity layer, a high temperatureresisting layer is attached to the upper end of the low temperature resisting layer, an antibacterial layer is attached to the upper end of the high temperature resisting layer, and an flame retardinglayer is attached to the upper end of the antibacterial layer. According to the 3D blowing membrane, a common PVC material is replaced by a TPU material, so that the comprehensive performance of theblowing membrane is improved, and the TPU material is non-poisonous and environmentally friendly, has incomparable characteristics compared with other plastics and natural materials, can significantlyenhance characteristics of the strength, the tenacity, wear resistance, ageing resistance, weather change resistance and the like of the blowing membrane and products of the blowing membrane, and then is more suitable for being used for production and lives.
Owner:瑞年科技(广东)有限公司

Method for purifying panaxoside compound-K by applying macroporous resin

The invention relates to a method for separating and purifying a panaxoside compound-K from microorganism zymocyte by applying macroporous resin for preparing a raw medicine. The purifying yield reaches more than 72 percent, and the content of the panaxoside compound-K in a product is more than 96 percent. The method mainly comprises the following steps of: adding ethanol into zymocyte for extracting and concentrating; decoloring by active carbon and filtering; after adding water into filter liquor for diluting, leading the filter liquor to pass through a macroporous resin chromatographic column; washing by a low-concentration organic solvent aqueous solution for removing pigment and high-polarity saponin; eluting by a high-concentration organic solvent aqueous solution to obtain a panaxoside compound-K component; and finally crystallizing to obtain the panaxoside compound-K raw medicine with the content of more than 96 percent. The invention can provide a great amount of qualified raw medicine samples for the pharmaceutical development of the panaxoside compound-K.
Owner:ZHEJIANG HISUN PHARMA CO LTD
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products