The invention discloses an industrial synthesis method of high-thermal-stability terminated
polysulfone resin. The industrial synthesis method comprises the following steps: adding a
solvent into a reaction kettle under
nitrogen filled protection, then increasing the temperature to 60-80 DEG C, sequentially adding 4,4-dichlorodiphenyl
sulfone and
bisphenol A to be used as reaction monomers, wherein the content of
solid in the
system is 20-40%; adding a salt forming agent after the monomers are thoroughly dissolved, subsequently adding a water dividing agent, increasing the temperature to 180-190 DEG C, and carrying out
salt formation reaction for 1-2 hours; then increasing the temperature to 200-220 DEG C, carrying out constant-temperature
polymerization reaction for 5-6 hours, adding a terminating agent, continuing to react for 10-30 minutes to obtain a polymerized
adhesive liquid; and cooling, crushing, filtering, washing and
drying the polymerized
adhesive liquid to obtain
polysulfone resin. The added terminating agent has an excellent terminating effect; the
system is not depolymerized; the terminated
polysulfone resin synthesized by the method is high in
thermal stability and low in gloss; and the process can be used for greatly shortening the reaction time, improving the productivity and widening the application field of the products.