The invention discloses a medical
magnetic hyperthermia copper-
nickel alloy and a preparation method thereof. The medical
magnetic hyperthermia copper-
nickel alloy is prepared from the following
raw material formula in percentage by weight: 15-25% of Cu, 50-60% of Ni, 0.05-0.08% of Sn, 1-1.3% of Fe, 0.01-0.015% of B, and 0.01-0.02% of Li; and during preparation, firstly, Cu, Ni and Fe raw materials are milled, subjected to vacuum
smelting, and cooled to 1200-1350 DEG C, Sn, B and Li are added, uniform electromagnetic mixing is conducted,
water cooling is conducted to the
room temperature, andan
alloy ingot is obtained; the alloy
ingot is turned into fines and then crushed to obtain alloy
powder;
vacuum sintering is conducted after
extrusion molding; and homogenization treatment is conducted. The produced
copper-
nickel alloy is fine and uniform in grain, can be used for tumor
hyperthermia, magnetic induction thermoseed materials processed through the copper-
nickel alloy is good in compactness, in an alternating
magnetic field, the thermal production capability is high, thermal distribution is uniform, and the self
temperature control property and the good
biocompatibility of magnetic induction thermoseeds are further retained.