The invention provides a preparation method of a
tourmaline / magnetic
chitosan microsphere treatment agent which is prepared by dissolving and uniformly mixing mixed
powder of
tourmaline and magnetic
chitosan microspheres in
sodium alginate and
polyvinyl alcohol, and solidifying and balling. The magnetic
chitosan microsphere is prepared by using superparamagnetic ferroferric
oxide, 1 to 10 weight percent of chitosan
acetic acid liquid,
liquid paraffin, Span-80 and
glutaraldehyde as reaction materials through an
emulsion crosslinking method, wherein the
mass ratio of the superparamagnetic ferroferric
oxide to the chitosan
acetic acid liquid is 1:(1-10), the volume ratio of the
liquid paraffin to the Span-80 is (10-100):1, the volume ratio of the chitosan
acetic acid liquid of superparamagnetic ferroferric
oxide to mixed liquid of paraffin-Span-80 is 1:(1-10), and the volume ratio of the mixed liquid of superparaferroferric oxide, paraffin and Span-80 to
glutaraldehyde is (5-50):1. According to the water treating agent, the removal rate of volatile
phenol in water is between 80 and 90 percent, the removal rate of
chromium in water is 93 percent; and the magnetic
chitosan microsphere treating agent has the advantages of large adsorption capacity, high purification efficiency, low cost, regeneration, no
toxicity, no
pollution to environment and the like.