The invention belongs to the technical field of building materials, and particularly relates to real stone
lacquer and a preparation method and a construction method thereof. The real stone
lacquer isprepared from sealing priming
lacquer, middle layer lacquer and finish lacquer, wherein the sealing priming lacquer is prepared from the following raw materials in parts by weight: 30 to 36 parts ofalkali resistant
emulsion, 8 to 12 parts of
silicon sol, 0.8 to 1.2 parts of texanol, 0.8 to 1.2 parts of
ammonium hydroxide and 50 to 60 parts of deionized water; the middle layer lacquer is preparedfrom the following raw materials in parts by weight: 180 to 220 parts of
emulsion, 600 to 800 parts of natural color sand, 8 to 12 parts of texanol, 1 to 2 parts of
ammonium hydroxide, 12 to 18 partsof thickening agents, 1 to 3 parts of antifoaming agents, 1 to 3 parts of sterilizing agents and 60 to 80 parts of deionized water; the finish lacquer is prepared from the following raw materials inparts by weight: 600 to 800 parts of
emulsion, 200 to 400 parts of deionized water, 2 to 4 parts of antifoaming agents and 1 to 2 parts of
ammonium hydroxide. The real stone lacquer has the advantagesthat the performance of water-resistance, salt-resistance and alkali-resistance is high; the reasonable color sand particle size grading is used, so that the sand falling phenomenon is obviously reduced; in addition, the preparation and construction methods are simple and are suitable for large-scale popularization and use.