The invention discloses a PP (
polypropylene) thin film. The PP thin film is prepared from components in a
raw material formula in parts by weight as follows: 50-60 parts of PP random copolymers, 15-20parts of PP block copolymers, 8-10 parts of
polyethylene, 7-10 parts of
calcium carbonate as a filling agent, 2-3 parts of glass fibers, 3-5 parts of talcum
powder, 1-2 parts of
silicon dioxide as alubricant, 1-2 parts of
carbon black as a coloring agent, 6-8 parts of amino resin and 13-15 parts of octadecanol. The formula with a reasonable ratio is adopted, new components including the glass fibers, the talcum
powder,
silicon dioxide,
carbon black, amino resin and the like are added to the
raw material formula, the ratio of the components is reasonably defined, so that by the aid of the ingenious component ratio, not only is integration of the components greatly improved, but also performance of the components is unexpectedly improved, finally, a product has the advantages of being goodin resistance to heat, acid and base, resistant to wear, light, non-toxic,
odor-free and the like, and
tear resistance,
oxidation resistance,
corrosion resistance and smoothness of the product are improved dramatically.