The invention discloses a preparation method and a product of
pulverized fuel ash desulfurized
gypsum rock
wool. The rock
wool is prepared from the following formula materials: 49% to 52% of
pulverized fuel ash, 48% to 50% of desulfurized
gypsum and 3% to 5% of waste glass, wherein the
pulverized fuel ash is wet discharged ash with the
natural water content of 12% to 18%; and the desulfurized
gypsum has the
natural water content of 10% to 13%. The preparation method comprises the following steps: weighing the materials according to proportions of the material formula; storing the pulverized fuel ash, the desulfurized gypsum and the smashed waste glass in a
silo and carrying out mechanical agitation so as to obtain a dried mixed material; carrying out aging, roll
grinding and briquetting on the dried mixed material and then naturally hardening so as to form lump materials; adding the hardened lump materials and
coke into a
cupola furnace according to the weight ratio of the
coke to the lump materials being 1 to 4, blowing hot air into the
cupola furnace so as to melt the mixed material to form a
silicate solution, and throwing the
silicate solution in a
centrifuge so as to obtain fibrous materials; and feeding the fibrous materials into a
settling chamber by virtue of high-pressure air, and delivering the fibrous materials by virtue of a net conveyor so as to form the pulverized fuel ash desulfurized gypsum rock
wool. According to the method, the
thermal insulation efficiency of the prepared rock wool reaches 97%, so that the
utilization rate of the pulverized fuel ash and the desulfurized gypsum is improved.