The invention relates to a modified formula for enhancing rapidly-dried silica
sol. The technical scheme is that: the modified formula consists of the following components in part by weight: 8,500 to 9,800 parts of silica
sol, 100 to 1,200 parts of
emulsion, 80 to 160 parts of
fiber, and 20 to 180 parts of antifoaming agent. The modified formula has the advantages that: by using the interpenetrating and complementary characteristics of the silica
sol and the
emulsion, coatings coated on the surface of a
wax mold are in net distribution, the
wet strength of the coatings is improved, and the next-layer
sizing agent can be applied to the incompletely dried upper-layer
sizing agent; by using the water conduction function of the
fiber, the water inside and outside the coatings is balanced, the inner stress is reduced, the mold shell
cracking probability is reduced, the
evaporation of the water is accelerated, and the
drying time is shortened; an ultra-
micro gap of the
fiber formed by high temperature
carbonization can reduce the retained strength of the mold shell, also can improve the air permeability of the mold shell, and comprehensively improves the quality of
casting products; and the period of shell making technology is shortened from 5-7 days to 1-2 days.