The present invention relates to an oriented
silicon steel strip with
diagonal stripes, and a production method thereof. The production method comprises: adopting a conventional production method to obtain an oriented
silicon steel
decarburization annealing steel strip; adopting a roll
coating or
spray coating method to coat a separation agent on the
decarburization annealing steel strip, such that the coated pattern of the separation agent and the steel strip length direction present the
angle alpha, wherein the
angle alpha is more than or equal to 10 DEG and is less than or equal to 90 DEG or the
angle alpha is more than or equal to -90 DEG and is less than or equal to -10 DEG, preferably the angle alpha is more than or equal to 30 DEG and is less than or equal to 90 DEG or the angle alpha is more than or equal to -90 DEG and is less than or equal to -30 DEG, the width of the coated pattern is 0.5-10 mm, and the
height difference between the deep position and the shallow position of the coated pattern is 0.1-3 mm; and carrying out high temperature annealing,
coating of an insulating
coating and hot stretching annealing to obtain the oriented
silicon steel finished product with
diagonal stripes. According to the present invention, with the separation agent for forming the
diagonal coated pattern on the steel strip surface, the air permeability of the steel coil during the high temperature annealing can be improved, the
water vapor in the high temperature annealing coil can be rapidly discharged, the defective product
reduction rate that the bottom layer defects, wrinkles and edge
waves and other defects are reduced is improved, and the bottom layer
color difference and the finished product strips
color difference are significantly improved, such that the product quality of the oriented silicon steel can be increased under the premise of no significant increase of the cost.