The invention discloses an environment-coordinating method for preparing
titanate piezoelectric
ceramic powder, and the method is characterized in that
lactic acid is chelating agent, swelling agent and pore-forming agent,
sol is prepared under the normal temperature by utilizing a
sol-
gel method, after the pH value is adjusted, the
sol is vacuum concentrated or removed with
solvent under
constant pressure to obtain gel, the gel is processed through unique swelling process and
spontaneous combustion way under the temperature of 180 DEG C to 200 DEG C to obtain a nano pyrophoric material, and the pyrophoric material is pre-burned to obtain nano
powder under the temperature of 550DEG C to 600DEG C; and the
powder is processed through procedures such as granulating, tabletting, plastic releasing and the like to obtain a green sheet, the green sheet is sintered for 1 to 2h under the condition of 950DEG C to 1025DEG C to obtain a
ceramic sheet, and the
ceramic sheet is polarized in normal-temperature
silicon oil to obtain the
titanate piezoelectric ceramic powder after standing. The method has important practical significance for traditional piezoelectric ceramic production process to realize high quality, low
energy consumption, low cost and environmental friendliness; and meanwhile, an important innovation effect for the
titanate compound application field seeking no conglobation and having ultra-large specific surface area can be achieved.