The invention belongs to the field of alloy material, relating to no-co ferrous alloy, in particular to no-co ferrous alloy for enhancing material of the sealing face of a nuclear power valve. The no-co ferrous alloy powder composition contains the following ingredients by weight percent: 20.5%-21.5% of Cr, 3.0%-3.5% of Ni, 3.0%-3.5% of Mn, 2.0%-2.5% of Si, 0.9%-1.0% of C, 1.5%-2.0% of Mo, 0.7%-1.2% of W, 0.3%-0.5% of V, P is less than or equal to 0.02%, S is less than or equal to 0.02%, 0.5%-1.0% of Y and the balance of Fe. The no-co ferrous alloy powder composition contains no noble metal of Co, at the same time, since laser cladding technology is adopted to prepare the coating, the microhardness of the cladding layer is 1.6-1.8 times of that the stainless steel matrix. The no-co ferrous alloy powder composition has excellent high-temperature abrasion performance and high-temperature corrosion resistance, so the no-co ferrous alloy powder composition can prolong the service life of the valve.