The invention relates to the technical field of
anode oxidation solution formulas and
anode oxidation processes, in particular to a
ceramic anode oxidation solution and a
ceramic anode oxidation process. The
ceramic anode oxidation solution per
liter comprises, by
mass concentration, 5-100 g of
titanium potassium oxalate, 1-30 g of additives A, 1-30 g of additives B and 1-20 g of additives C. The ceramic
anode oxidation process comprises the steps that firstly, aluminum
alloy materials to be subjected to ceramic anode oxidation are put in a reaction tank filled with the ceramic anode oxidation solution; and then the ceramic anode oxidation solution is heated to be at 15-60 DEG C, the
voltage of 20-120 V is introduced, oxidation is conducted for 15-80 min, and the ceramic anode oxidation step is finished. The film thickness generated by a ceramic anode is in a
tree root shape, the ceramic anode has incomparable
hardness advantages compared with an ordinary anode, the surface color decoration range of an aluminum
alloy ceramic oxidation film is enlarged, and the beautiful
surface enamel sense is kept. Meanwhile, the ceramic anode has the firm and color appearance meeting different decorative requirements, and has good abrasion resistance,
corrosion resistance and
weather resistance properties in the use process, the
process conditions are simple, and implementation is convenient.