The invention provides a composite
corrosion inhibition antisludging agent for ultralow rigidity circulation cooling water. The composite
corrosion inhibition antisludging agent comprises the following raw materials in parts by weight: 5-15 parts of amino trimethylene phosphonic acid, 5-15 parts of
hydroxyethylidene diphosphonic acid, 1-15 parts of
diethylenetriamine pentamethylene phosphonic acid, 5-15 parts of hydrolytic
polymaleic anhydride, 2-15 parts of terpolymer, 2-20 parts of heptahydrate, 0.1-2 parts of hydroxy
benzotriazole and 3-79.9 parts of pure water. The hydroxy
benzotriazole is added after the amino trimethylene phosphonic acid, the
hydroxyethylidene diphosphonic acid, the
diethylenetriamine pentamethylene phosphonic acid, the hydrolytic
polymaleic anhydride and the terpolymer are stirred and mixed; and the composite
corrosion inhibition antisludging agent is obtained by adding the water and the heptahydrate until the hydroxy
benzotriazole is entirely dissolved. The hydrolytic
polymaleic anhydride and the terpolymer used by the invention have a good
diffusion effect, and can effectively prevent carbonates, phosphates and the like from being deposited and scaled. Meanwhile, the hydrolytic polymaleic anhydride and the terpolymer belong to a non-
phosphate monomer, so that the agent
phosphate content is reduced. Therefore, the composite corrosion inhibition antisludging agent is beneficial to
environmental protection.