The invention relates to high-count combed
camel hair woven
yarn. The high-count combed
camel hair woven
yarn is formed by blending 50% of
camel hair fiber and 50% of water-soluble vinylon
fiber, wherein the metric count of actually-spun
yarn is 100 Nm / 2, the metric count of vinylon-dissolved yarn is 200 Nm / 2, the single yarn twist coefficient is 105, and the doubled yarn twist coefficient is 87. A manufacturing method of the yarn includes the steps that oiling and life preserving are conducted on camel hair
fiber and
pile, combed camel hair strips are formed through the
carding procedure, the gilling procedure, the
combing procedure and the gilling procedure, the camel hair strips are mixed, oiling and life preserving are conducted on the mixed strips, and drawing silver suitable for
spinning production is manufactured after the strips and 50% of vinylon strips are mixed, combined and combed; the camel hair and vinylon fiber blended yarn is manufactured through the other seven procedures of pre-
spinning, the spun yarn procedure, the
spooling procedure, the doubling procedure, the two-for-one twisting procedure, a product is formed by the yarn through beaming and weaving, and the high-count combed camel hair woven yarn is obtained after water-soluble vinylon fiber is dissolved and removed in the normal washing and contracting process. The input-output ratio of the produced vinylon-treated high-count camel hair blended woven yarn is higher than that of normal pure camel hair yarn, and fabric is lighter and thinner.