Belongs to the technical field of
wood processing. In order to solve the problem that an
adhesive agent is adopted in an existing reconstituted
veneer, and consequently, poisonous and harmful volatile matter is released, the preparing method of the glue-free reconstituted
veneer comprises the steps that a fast-growing
wood veneer is subjected to delignification by using a delignification solution to obtain a delignified wood sample; 80% of water in the delignified wood sample is removed through cold pressing; and after hot-pressing
drying, a glue-free reconstituted
veneer is obtained. According to the preparing method, hydroxyl on the surface of
cellulose and
hemicellulose is exposed through delignification, a multiple
hydrogen-bond network is formed under pressure, and high
mechanical strength and high size stability of the reconstituted veneer are given. In the preparing method, no
adhesive agent is used, the reconstituted veneer is low in cost, simple in process and short in time, zero volatile of
formaldehyde is really realized; the problems are solved that a great amount of the
adhesive agent is used in artificial timbers, the indoor environment is polluted, and the
human body health is harmed; and the glue-free reconstituted veneer has a higher market value.