The invention provides an In2S3 / MIL-53(Fe) efficient photocatalytic
composite material, a preparation method and application. The
mass ratio of In2S3 to MIL-53(Fe) is (10-30):1. The preparation methodcomprises the following steps: step 1, mixing InNO3 hydrated with 4.5H2O with MIL-53(Fe), and adding the mixture into water; step 2, dissolving L-
cysteine in the same amount of water as that in the step 1; step 3, dropwise adding the solution obtained in the step 2 into the
mixed solution obtained in the step 1 under a stirring condition, conducting stirring at
room temperature, transferring a formed mixture into a high-pressure reaction kettle with a
polytetrafluoroethylene lining, and carrying out sealed reaction; and step 4, naturally cooling the reacted
mixed solution obtained after the reaction in the step 3 to
room temperature, repeatedly conducting washing with water and absolute ethyl
alcohol to remove impurities from the product, and conducting
drying to obtain the In2S3 / MIL-53(Fe) high-efficiency photocatalytic
composite material. According to the efficient photocatalytic
composite material disclosed by the invention, In2S3 is introduced, so that the
diameter of an MIL-53(Fe) microrod is increased, the surface is rougher, more active sites can be provided, and the photocatalytic activity is favorably improved.