The invention relates to a wear-resistant drag
reducer for
drilling fluid and a preparation method thereof. The wear-resistant drag
reducer is characterized in that a formula of the wear-resistant drag
reducer is prepared from the following main raw materials:
vegetable oil acid, cotton seed oil,
sulfur powder, diethanol amine and
kerosene; the auxiliary raw materials comprise
tributyl phosphate, organic soil and T323 anti-wear
reagent at extreme pressure. The wear-resistant drag reducer for
drilling fluid comprises the following components in percentage by weight based on the total amount of the drag reducer: 7-13 percent of
vegetable oil acid, 26-31 percent of cotton seed oil, 6-11 percent of
sulfur powder, 3-5 percent of diethanol amine, 27-29 percent of
kerosene and 12-17 percent of auxiliary materials and other materials. The method for preparing the wear-resistant drag reducer for
drilling fluid comprises a sulfonation reaction, an amidation reaction and a mixed reaction. When the wear-resistant drag reducer is used for drilling, the drag reducer can be adsorbed to the surface of a drilling tool preferentially, a dense high-strength protective film is generated, the lubricating property of the drilling fluid is reduced, the friction and wear of the
metal surface are reduced, an extreme pressure
lubrication coefficient and a mud cake
adhesion coefficient of the drilling fluid are effectively reduced, blockage and other accidents in the drilling process are reduced.