The invention provides a high-performance historic site
repair material and a preparation method thereof. The
repair material comprises the following raw materials: 191-287 parts of sticky rice pulp, 115-185 parts of
lime, 0-4 parts of brown granulated
sugar, 344-398 parts of fine aggregates, 204-268 parts of complex mineral admixture, 11-12 parts of reinforcing agent, and 0-19 parts of mineral
pigment. The invention further provides a preparation method of the
repair material. The preparation method comprises the following steps: weighing all the
raw material according to weight, and forcibly stirring evenly to obtain the repair material.
Amylopectin in the sticky rice pulp is a highly branched
macromolecule, the setting and hardening processes of the
lime and the
pozzolanic reaction of the complex mineral admixture are influenced, the strength development of the material is similar to
biomineralization process, and a
microstructure formed in the process endows the repair material with higher strength and
toughness. Furthermore, the material has good compatibility with materials of a historic site body.