The invention discloses a wear-resistant
elbow material. The formula of the wear-resistant
elbow material comprises the following components: 3.3 to 3.7 percent of carbon, 2.3 to 2.8 percent of
silicon, 0.5 to 1.0 percent of
manganese, 0.4 to 1.0 percent of
chromium, 0.03 to 0.06 percent of
phosphorus, 0.01 to 0.02 percent of
sulfur, 0.03 to 0.05 percent of
magnesium, 0.01 to 0.02 percent of
cerium, 0.3 to 1.0 percent of
vanadium, 0.3 to 1.0 percent of
neodymium, 4 to 6 percent of aluminum
oxide, 3 to 6 percent of
titanium diboride and the balance of iron. The invention further discloses a preparation process of the wear-resistant
elbow material. The preparation process comprises the following steps of quantitative weighing,
raw material smelting, spheroidizing treatment and
inoculation treatment,
casting molding,
quenching, wear-resistant hard phase overlaying and dip-
coating. The wear-resistant elbow material has the beneficial effects that the prepared wear-resistant elbow material is greatly improved, the
wear resistance of an elbow is improved through a wear-resistant hard phase formed by mixing aluminum
oxide and
titanium diboride, and the inner wall of the elbow is dip-coated with a layer of Teflon to reduce material adhesion, so that the wear-resistant elbow is not only suitable for conveying hard substances, but also suitable for conveying
soft materials.