The invention discloses micro-expansion
fiber reinforced concrete for a steel-concrete combined
beam bridge panel wet joint and a preparation method of the micro-expansion
fiber reinforced concrete, and relates to the preparation field of the micro-expansion
fiber reinforced concrete. The micro-expansion
fiber reinforced concrete comprises gel materials (
cement,
coal ash,
slag powder and an expanding agent), aggregate, reinforcing materials, imitated steel fibers, a
water reducer and water, wherein the 28
compressive strength of the micro-expansion
fiber reinforced concrete is not lower than 69.0MPa, the 28d
breaking strength of the micro-expansion
fiber reinforced concrete is not lower than 7.0 MPa, the 28d splitting tensile strength of the micro-expansion fiber reinforced concrete is not lower than 5.0 MPa, the 28d elasticity modulus of the micro-expansion fiber reinforced concrete is not lower than 36.0 GPa, the
cracking resistance level of the micro-expansion fiber reinforced concrete reaches L-IV level, the 28d bending
toughness index I20 of the micro-expansion fiber reinforced concrete is not lower than 8, the 56d
chlorine ion diffusion coefficient of the micro-expansion fiber reinforced concrete is lower than 4.0*10<-12>m<2> / s, the 21d shrinkage percentage of the micro-expansion fiber reinforced concrete is lower than 200*10<-6>. By using the preparation method, the
shrinkage cracking of the micro-expansion fiber reinforced concrete can be effectively avoided, so that the reinforced concrete is relatively compact. The micro-expansion fiber reinforced concrete disclosed by the invention is relatively high in strength, relatively low in shrinkage percentage, good in bending
toughness and durability, relatively low in cost and conveniently to widely use.