The invention discloses a preparing method of a
ceramic bonding agent CBN (Cubic
Boron Nitride)
grinding wheel with a precisely adjustable and controllable
hardness attenuation value. The preparing method comprises the following steps that: 16 to 20 weight percent of
boric acid, 9 weight percent of
sodium carbonate, 5 weight percent of
potassium carbonate, 8 weight percent of aluminum
oxide, 4 weight percent of
titanium dioxide, and 54 to 58 weight percent of
silicon dioxide are pretreated; bonding agents are prepared through
smelting; the bonding agents are crushed; the bonding agents are subjected to ball milling; 15 to 23 weight percent of bonding agent
powder, 72 to 80 weight percent of CBN
grinding materials, 3 weight percent of yellow
dextrin powder and 2 weight percent of deionized water are poured into a
grinding jar, ball milling is carried out, and
grinding wheel forming materials are prepared; a
grinding wheel is formed after pressurizing and
drying; the
grinding wheel is sintered; a
buffer solution is prepared; and the
buffer solution is utilized for adjusting and controlling the
hardness of the grinding wheel, and the
ceramic bonding agent CBN grinding wheel with the precisely adjustable and controllable
hardness attenuation value is prepared. The preparing method has the advantages that the hardness of the prepared
ceramic CBN grinding wheel is precise and controllable, the ceramic CBN grinding wheels which have different hardness and are suitable for being used for grinding different materials are obtained, and the grinding performance of the ceramic CBN grinding wheel is improved.