The invention provides a preparation technology of
dolomite sand, which comprises the following steps: (1)
dolomite with the particle size of 10-80 mm is selected, wherein the
dolomite comprises the following chemical components in parts by weight: larger than or equal to 0.29 part of SiO2, larger than or equal to 0.1 part of Fe2O3, larger than or equal to 0.15 part of Al2O3, larger than or equal to 30.06 parts of CaO, and larger than or equal to 22.7 parts of MgO, in addition, the dolomite is
cut down for 40-50 according to the circumference, (2) low-ash
hard coal is adopted as fuels to be calcinated in a high temperature shaft
kiln, wherein the calcinating temperature is 1,750-1,850 DEG C; an intermittent
oxygen-enriched
calcination way is adopted, wherein one-time drawing out of the
kiln is carried out in calcinating for 4-6 hours, and the times of entering in and drawing out of the
kiln is 4-6; (3) the calcinated dolomite sand comprises the chemical components in parts by weight: 1.11-1.18 parts of SiO2, 0.56-0.6 part of Fe2O3, 0.45-0.64 part of Al2O3, 56.94-57.67 parts of CaO, and 39.93-40.21 parts of MgO, in addition, the calcinated dolomite sand is
cut down for 0.28-0.43 according to the circumference, and has
volume density of higher than or equal to 3.2. The dolomite sand is manufactured by one-step calcinating, and on one hand, the consumption of raw materials and fuels are enabled to be remarkably reduced, on the other hand, the preparation technology is greatly simplified, therefore, the production cost is lowered greatly.