The invention relates to a micro-fine particle
cassiterite flotation method. The micro-fine particle
cassiterite flotation method comprises the steps that
tin-containing materials are prepared into pulp, and
ammonium bicarbonate is added in the pulp; then an adjusting agent, collecting agents and a
foaming agent are added, wherein the collecting agents comprise
naphthalene hydroximic acid,
benzohydroxamic acid and oxidized
paraffin wax soap; and the pulp is subjected to roughing, and then
citric acid and
sodium fluosilicate are added into
tin rough concentrate for choiceness to obtain
cassiterite concentrate. The problems that the micro-fine particle cassiterite flotation
recovery rate is low, the concentrate grade is unsatisfactory, and the
impurity content is high are solved, and the
tin concentrate with the Sn content being larger than or equal to 35% and the
recovery rate being larger than or equal to 90% can be obtained; and compared with the prior art, the thin concentrate
recovery rate is increased by 15-20%, and the tin concentrate grade is improved by 10-15%. The low-carbon, environment-friendly, economical and efficient method for micro-fine particle cassiterite recovery through flotation is simple in technique, has the advantages that the material adaptability is high, using is safe and stable, the
reagent dosage is few, and
pollution is little, and has good application prospects.