The invention discloses a preparation method of
polyphenyl ether thioether sulfoxide. The
polyphenyl ether thioether sulfoxide comprises the following ingredients: 4,4'-dyhydroxy
diphenyl sulfide and 4,4'-dihalogen diphenylsulfoxide as the reaction
monomer of which the
mole ratio is 1: 1.02, 1.1-2.5mole / mole of 4,4'-dyhydroxy
diphenyl sulfide as the assistant, 0.1-0.5 mole / mole of 4,4'-dyhydroxy
diphenyl sulfide as the catalyst, 1000-2000ml / mole of 4,4'-dyhydroxy diphenyl
sulfide as the
solvent, and 300-500ml / mole of 4,4'-dyhydroxy diphenyl
sulfide as the azeotropy dehydrating agent. The process comprises the following steps of: (1) adding the ingredients into a reaction contain and stirring under the protection of
nitrogen at the
room temperature, rising the temperature, heating, and dehydrating, ending the
dehydration when the temperature reaches 130-150 DEG C, subsequently rising the temperature to 170-220 DEG C and carrying out the
polymerization reaction, when the reaction is ended, cooling naturally to the
room temperature and stopping stirring; and (2) pouring the mixture liquid formed by the
polymerization reaction into precipitating agent, precipitating and filtering so as to obtain a
filter cake, washing the
filter cake and
drying in vacuum so as to obtain the
polyphenyl ether thioether sulfoxide; and the
structural formula is: (FORMULA).