The invention provides a production method of tissue compensation glue for cancer radiotherapy, the preparation method comprises the following steps: 1, weighing solid paraffin, low-density polyethylene, a styrene-maleic anhydride copolymer and cross-linked povidone according to the mass ratio of 100: 2: 12-14: 3-7; S2, mixing the styrene-maleic anhydride copolymer with the cross-linked povidone,adding 1,4-dioxane for co-boiling, then cooling to 10-20 DEG C, keeping for 30-40 minutes, then adding hydroxylamine hydrochloride and sodium methoxide to react, then adding methylbenzene for co-boiling for 5 hours, filtering, washing filter residue with diethyl ether and water, and carrying out vacuum drying on the filter residue until the filter residue reaches constant weight to obtain a synergist; S3, mixing and injecting the solid paraffin, the low-density polyethylene and the synergist into a mold, and performing molding and demolding to obtain the tissue compensation adhesive for cancerradiotherapy. The production method provided by the invention has the advantages of simple operation and one-time forming, and the produced tissue compensation glue can be applied to cancer radiotherapy and is good in adhesion to skin.