The invention discloses a preparation method for a
cobalt-loaded ordered
mesoporous carbon material and an application of the
cobalt-loaded ordered
mesoporous carbon material in the process of catalyzing oxone to degrade
rhodamine B in
wastewater, and belongs to the technical fields of synthesis of
mesoporous carbon materials and organic
wastewater treatment. The key points of the technical schemeare as follows:
melamine is used as a
nitrogen source, F127 is used as a template agent,
melamine-phenolic resin balls are prepared through a
polycondensation reaction of
resorcinol and formaldehydeby adopting a hydrothermal method, high-temperature
calcination is performed, so that a mesoporous carbon carrier is obtained, and the mesoporous carbon carrier and a
cobalt sulfate solution are further subjected to a
hydrothermal reaction to synthesize the cobalt-loaded ordered mesoporous carbon material, wherein with the change of the ratio of the raw materials, a series of cobalt-loaded orderedmesoporous carbon materials can be obtained, so that the efficiency of catalyzing the oxone to degrade the
rhodamine B in the
wastewater is effectively improved. The cobalt-loaded ordered mesoporouscarbon material prepared by the method of the invention can effectively remove the
rhodamine B in the
water body, has large removal capacity, large adsorption capacity, high removal efficiency and convenient operation, is insoluble in the
water body, can be recycled, and has good adsorption catalytic performance.