The invention relates to a heat-resistant ASA resin composition with tiger
wrinkle defect eliminated and a preparation method thereof. The heat-resistant ASA resin composition is prepared from following raw materials, by weight: 30-50 parts of ASA rubber
powder, 30-60 parts of SAN resin, 5-15 parts of a tiger
wrinkle defect eliminating agent, 5-20 parts of a heat-resistant agent and 0.5-1.5 parts of a
processing aid. The preparation method comprises the following steps: stirring and fully mixing the raw materials in a high-speed mixing
machine, feeding the mixture into a double-screw extruder through a metering device to melt and composite the mixture through transportation, shear and mixing by means of screw rods, and performing
extrusion, bar drawing, cooling and granule
cutting to prepare the heat-resistant ASA resin composition. The method is easy to carry out. The tiger
wrinkle defect on a workpiece during an
injection molding process can be completely avoided by means of the ASA resin composition. The resin composition also is excellent in anti-
impact, heat-resistant and such comprehensive performance, and is very suitable for being used as automobile exteriors, such as automobile gratings, columns, empennage decorative plates and the like.