Warm-mixed asphalt mixture and preparation method thereof

The invention relates to a warm-mixed asphalt mixture and a preparation method thereof. The warm-mixed asphalt mixture is mainly applied to new construction and maintenance of high-grade roads and common roads, and is particularly suitable for cities, parks, tunnels and the like with high environmentally-friendly requirements. The warm-mixed asphalt mixture mainly comprises about 92.4-96.5 percent by weight of mineral, about 3.4-7.5 percent by weight of asphalt cement and 0.05-1.0 percent by weight of chemical modified adhesive cement. The preparation method comprises the following steps of: simultaneously pumping the chemical modified adhesive cement and the hot asphalt cement to the spraying port of a foam generator, fully mixing to generate a foam-containing hot asphalt mixture, spraying the foam-containing hot asphalt mixture into a mixing pan, and further mixing the foam-containing hot asphalt mixture and the hot mineral to form the warm-mixed asphalt mixture. The chemical modified adhesive cement can effectively reduce the mixing, spreading and rolling temperature of the asphalt mixture, and solves the problems of environmental pollution, high energy consumption, asphalt ageing regression and the like. By selecting high-concentration cationic chemical modified latex as a matrix stock of the chemical modified adhesive cement and simultaneously matching a proper proportion of cationic surfactant with lubricating effect and peeling resistance, the influence of the conventional warm-mixed asphalt additive on poor reducing performance and poor adhesive performance of the asphalt cement is solved, and the properties of the warm-mixed asphalt mixture such as water damage resistance, rutting resistance, fatigue resistance, low temperature resistance and the like are improved.
Owner:PETROCHINA CO LTD

Warm-mix asphalt additive and preparation method thereof

The invention relates to a warm-mix asphalt additive and a preparation method thereof. The additive comprises the following components in percentage by weight: 87 to 98 percent of chemical modification latex, 0.5 to 12 percent of lubricative and peeling resistant cation surfactant and 0.1 to 2.0 percent of acid. The method comprises the following steps of: heating the chemical modification latex to the temperature of between 40 and 80 DEG C with stirring, and dripping 0.1 to 0.5 percent of acid slowly; adding the lubricative and peeling resistant cation surfactant, stirring fully, and dispersing uniformly; and continuing to drip 0.1 to 1.5 percent of acid slowly, stirring uniformly, keeping the temperature of between 40 and 80 DEG C and storing for later use. By the warm-mix asphalt additive and the preparation method, the viscosity of asphalt binders during mixing can be reduced effectively, the reduction performance of asphalt cements and adhesivity between the asphalt cements and aggregates can be improved, the water damage resistance and durability of warm-mix asphalt mixtures can be improved, the tensile strength of asphalt can be improved, and the rutting resistance, fatigue resistance and low temperature resistance of the warm-mix asphalt mixtures can be enhanced.
Owner:PETROCHINA CO LTD +1

Polyurethane modified asphalt waterproof roll and production method thereof

InactiveCN108099306AStable hydrolysisStable light fadeSynthetic resin layered productsLaminationWater leakageBituminous waterproofing
The invention relates to a polyurethane modified asphalt waterproof roll. The polyurethane modified asphalt waterproof roll is of a five-layer structure which comprises, from top to bottom, a top isolating layer, an upper modified asphalt layer, a padding layer, a lower modified asphalt layer and a bottom isolating layer, wherein the upper modified asphalt layer and the lower modified asphalt layer are prepared from modified asphalt. The polyurethane modified asphalt waterproof roll is greatly improved in tearing strength, adhesion, water resistance, aging resistance and the like, has high elongation at break, and overcomes the disadvantages of tedious preparation, weak adhesion and the like of conventional waterproof rolls. A production method for the polyurethane modified asphalt waterproof roll is simple. As the polyurethane modified asphalt waterproof roll is applied to a building, a contact surface of the polyurethane modified asphalt waterproof roll and the base surface of the building has good bonding strength and waterproof effect, so the waterproof roll is effectively prevented from water seepage and water leakage.
Owner:GUANGXI WUXUAN JINPAI WATERPROOF MATERIAL SCI & TECH CO LTD

Hot-melt traffic paint and preparation method thereof

ActiveCN107573777AReduce marking cracks and even fall offImproves compression and crack resistanceAntifouling/underwater paintsLuminescent paintsCorrosionVisibility
The invention relates to the technical field of traffic paint and in particular relates to hot-melt traffic paint and a preparation method thereof. According to the paint, multiple functional aids areselected to be combined to be used, the wear resistance, cracking resistance, corrosion resistance and antifouling property of the paint are improved. The primer paint can be well combined with the ground, so that pavement micro-pores are closed, the variation of the pavement and traffic line deformation under high-temperature or high-pressure conditions can be balanced, cracking even drop of thetraffic line caused by the variation of the deformation is reduced, and the mind-set of improving the cracking resistance, drop and other inner performances of the traffic line by adjusting the components and doses of various aids in the paint only in the traditional paint is broken; coloring pigments and auxiliary luminous materials are added into intermediate paint layer to serve as a traffic sign luminous layer and are combined with the surface paint to be used; glass beads are added into the surface paint, so that the reflective refraction of the coating is improved. Due to rare-earth high polymer photoluminescence materials and nano fluorescent particles in the intermediate layer and the surface layer, the visibility of the traffic line is obviously improved.
Owner:WELL ROAD MACHINERY CO LTD

Road and bridge expansion joint structure

The invention discloses a road and bridge expansion joint structure. The road and bridge expansion joint structure comprises an inverted-T-shaped plate component with the bridge longitudinal cross section being in an inverted T shape. Two wing plates of the inverted-T-shaped plate component transversely extend into a base body of a bridge pavement layer. A web extends upwards to be flush with the upper surface of the bridge pavement layer. Each wing plate is sequentially provided with a cushion layer and a protection wear-resisting layer from bottom to top in a laying mode and is longitudinally connected with the bridge pavement layer. An expansion joint notch and the two sides of the expansion joint notch are filled with elastic layers to be sealed. The road and bridge expansion joint structure has the advantages of being convenient to construct, reasonable in design, high in efficiency, good in vehicle load bearing performance, good in elasticity, smooth and attractive in surface, and good in waterproofing, anti-aging, anti-fatigue, shock resistance and corrosion resistance. In accordance with the characteristics of an expansion joint, three materials of different components and matching ratios are adopted, layered pavement is conducted according to different stress conditions and states, good durability is achieved, construction is rapid and simple, and the expansion joint performance requirement can be well met.
Owner:孟献春

Asphalt cement doped with surface treated basalt fiber and crumb rubber

The invention discloses asphalt cement doped with surface treated basalt fiber and crumb rubber. The asphalt cement comprises the components in parts by mass as follows: 82.7-86.3 parts of matrix asphalt, 13.1-16.4 parts of the surface treated crumb rubber and 0.6-0.9 parts of the surface treated basalt fiber, and the mass sum of the components is 100, wherein a coupling agent solution is adopted for surface treatment of the basalt fiber and the crumb rubber, and the composition ratio of a coupling agent to water to ethanol for the coupling agent solution is 1:(3-6):(10-20). The asphalt cement is mainly applied to an asphalt pavement in an area with high temperature in summer, and can improve the anti-rutting capacity and anti-cracking capacity of the asphalt pavement effectively, reduce the maintenance cost of the asphalt pavement and prolong the service life of the asphalt pavement.
Owner:CHANGSHA UNIVERSITY OF SCIENCE AND TECHNOLOGY

Warm mix asphalt mixture and preparation method thereof

The invention discloses a preparation technology of a warm mix asphalt mixture. The warm mix asphalt mixture comprises 88-93 parts of mineral aggregate, 6-10 parts of modified warm mix asphalt and 1-2parts of fibers, wherein the modified warm mix asphalt comprises the following ingredients in parts by weight: 66-76 parts of matrix asphalt, 7.5-10 parts of rubber cracking oil, 6-8 parts of plasticcracking wax, 6-7 parts of alkene oil, 2-4 parts of a polymer, 2-4 parts of fatty acid and 0.5-1 part of an additive. The preparation technology comprises the steps of feeding the mineral aggregate heated to 120-140 DEG C into a blending cylinder, adding heated asphalt at 105-125 DEG C and a warm mix asphalt modifier, performing stirring 2-4 min, feeding the fibers, and performing blending for 0.5-1 min to form the warm mix asphalt mixture. The performance, such as water damage resistance, rut resistance and fatigue resistance, of the warm mix asphalt mixture are improved; when the warm mix asphalt mixture is applied to road construction, a service life of a road is effectively prolonged; and the preparation technology is simple and low in cost, has great economic and social benefits andmeets the characteristics of green ecology and sustainable development.
Owner:内蒙古高速公路集团有限责任公司

Heating system for epoxy asphalt steel bridge deck pavement and pavement method

The invention relates to a heating system for epoxy asphalt steel bridge deck pavement and a pavement method. The heating system can be used for controlling the operation temperature in the epoxy asphalt steel bridge deck pavement process, thereby shortening the curing time of epoxy asphalt, further greatly shortening a construction period and reducing the maintenance time before the opening to traffic. Simultaneously, the invention provides a pavement method using the heating system for epoxy asphalt steel bridge deck pavement; and the pavement method can enable the epoxy asphalt steel bridge deck pavement to be constructed in winter and can also be adopted in summer when fast curing is needed.
Owner:BEIJING BRIDGE RUITONG MAINTENANCE CENT +3

Polyurethane modified asphalt waterproof paint for buildings and production method thereof

The invention relates to a polyurethane modified asphalt waterproof paint, which is composed of the following raw materials by weight: 25-30 parts of a polyurethane prepolymer; 70-75 parts of 90# petroleum asphalt; 40-60 parts of water; 20-25 parts of polychloroprene latex; 4-7 parts of an emulsifier; 2-4 parts of polyvinyl alcohol; 1-3 parts of a coupling agent; 1-2 parts of polypropylene glycol;3-5 parts of trihexyl o-acetylcitrate; 0.1-0.5 part of pentaerythritol ester of hydogenated rosin; 1-3 parts of polyacrylamide; and 10-15 parts of modified nano calcium carbonate. The polyurethane modified asphalt waterproof paint prepared by the method provided by the invention has good film compactness and high stability, a waterproof layer formed by the waterproof paint in a building has largebonding strength with a building base surface and good waterproof effect, moreover, after modification, the product has substantially improved water tolerance, aging resistance, acid and alkaline resistance and the like, has a simple making process, and overcomes the disadvantages of tedious making, poor film compactness, poor waterproofness and aging resistance in previous water emulsified asphalt paint.
Owner:GUANGXI WUXUAN JINPAI WATERPROOF MATERIAL SCI & TECH CO LTD

High-viscosity high-elasticity modified asphalt produced from Bachaquero crude oil straight-run asphalt and preparation method thereof

The invention relates to high-viscosity high-elasticity modified asphalt produced from Bachaquero crude oil straight-run asphalt and a preparation method thereof. Raw materials include 85-90 parts by mass of matrix asphalt, 5-10 parts by mass of an SBS modifier, 1-2 parts by mass of extract oil, 2-4 parts by mass of a ductility improver and 0.1-0.3 part by mass of a stabilizer. The high-viscosity high-elasticity modified asphalt is low in cost, has the viscosity of more than 100000Pa.s at the temperature of 60 DEG C, is an asphalt binder with excellent performance and can be applied to bridge deck pavement, drainage road pavement and permeable pavement, the durability of an asphalt mixture can be effectively improved, the operating requirement of the drainage asphalt mixture can be completely met, and the blended asphalt mixture has excellent moisture damage resistance, rut resistance and scattering resistance.
Owner:FOSHAN GAOFU PETROCHINA FUEL ASPHALT

Warm-mixing epoxy asphalt mixture and preparation method thereof

ActiveCN106630760AImproved Marshall stabilityImproved anti-ruttingClimate change adaptationEpoxyAlkane
The invention discloses a warm-mixing epoxy asphalt mixture and a preparation method thereof. The warm-mixing epoxy asphalt mixture comprises the following components by weight percentage: 4.0-6.0% of warm-mixing epoxy asphalt, 1.0-3.0% of ore powder, and 91.0-95% of an aggregate; wherein, the warm-mixing epoxy asphalt mixture comprises a component A, a component B, and a component C, wherein the component A is warm-mixing asphalt, the warm-mixing asphalt comprises a warm-mixing agent and a matrix asphalt; the component B is an epoxy resin composition; and the component C is a curing agent. The preparation method of the warm-mixing agent comprises the following steps: under the effect of a catalyst, high-molecular alkane is reacted with a halogen simple substance to obtain an intermediate; aromatic hydrocarbons oil and a complex are uniformly mixed to obtain an aromatic hydrocarbons complexation component under effect of a second catalyst; and the aromatic hydrocarbons complexation component and the intermediate are reacted and slaked to obtain the warm-mixing agent. The epoxy asphalt mixture has good Marshall stabilization degree, rut resistance and water damage resistance capabilities.
Owner:CHINA PETROLEUM & CHEM CORP +1

Asphalt road

InactiveCN106223150AImprove flatnessTightness of compactionIn situ pavingsTemporary pavingsLow voltageSlag
The invention discloses an asphalt road, and belongs to the field of roads. The asphalt road comprises a roadbed, a subgrade and a road surface. The subgrade is arranged in the roadbed and is provided with a horizontal layered structure. The subgrade is provided with a first mixed slag layer, a rubble layer, a second mixed slag layer and a concrete layer from bottom to top, and a geogrid and low-voltage shielded wires are arranged in the second mixed slag layer. A plurality of solar photovoltaic modules are arranged in the middle of the road surface in the road extension direction, and the solar photovoltaic modules are connected with a photovoltaic inverter through the low-voltage shielded wires. The asphalt road has the characteristics of being high in flatness, capable of avoiding the circumstances of insufficient partial compaction degrees, serious temperature segregation and the like, good in road surface temperature sensing property, good in elasticity and ageing-resistant performance, not prone to melting or flowing at high temperatures, good in toughness and not likely to be cracked at low temperatures, capable of meeting the using requirements of high-grade roads, and capable of fully utilizing high temperatures of the road surface to conduct solar power generation.
Owner:江西省地质工程集团有限公司

Warm mixed epoxy asphalt, mixture containing same and preparation method thereof

The invention discloses warm mixed epoxy asphalt. The product comprises a warm mixed asphalt, an epoxy resin composition and a curing agent. The warm mixed asphalt comprises a warm mixing agent and matrix asphalt. The warm mixing agent is prepared by performing a sweating process by taking a byproduct polyethylene wax as a raw material. In the sweating process, oil soluble organic matters capable of decomposed to generate gas are pre-added into the byproduct polyethylene wax raw material, and micro-bubbles are formed in a wax layer by means of gas generated by the byproduct polyethylene wax which is heated, so that a liquid component is quickly discharged and separated; meanwhile, in the sweating process, the liquid component is carried out through the wax layer by means of the air flow to separate the solid component from the liquid component in a forced manner, so that the low molecular weight components in the raw material are removed more effectively. The warm mixing agent used in the product not only can play a warm mixing role on the asphalt, but also can improve the thermal stability of the asphalt, improve the anti-thermal aging property, reduce the fusing temperature of the asphalt and the viscosity at the temperature, and reduce the generation amount of harmful gas.
Owner:CHINA PETROLEUM & CHEM CORP +1

Warm-mixing epoxy asphalt mixture and preparation method thereof

The invention discloses a warm-mixing epoxy asphalt mixture and a preparation method thereof. The warm-mixing epoxy asphalt mixture comprises the following components by weight percentage: 4.0-6.0% of warm-mixing epoxy asphalt, 1.0-3.0% of ore powder, and 91.0-95% of an aggregate; wherein, the warm-mixing epoxy asphalt mixture comprises a component A, a component B, and a component C, wherein the component A is warm-mixing asphalt, the warm-mixing asphalt comprises a warm-mixing agent and a matrix asphalt; the component B is an epoxy resin composition; and the component C is a curing agent. The preparation method of the warm-mixing agent comprises the following steps: under the effect of a catalyst, high-molecular alkane is reacted with a halogen simple substance to obtain an intermediate; aromatic hydrocarbons oil and a complex are uniformly mixed to obtain an aromatic hydrocarbons complexation component; the aromatic hydrocarbons complexation component is added in the intermediate, under the catalysis effect of the complexation component, and the aromatic hydrocarbons complexation component and the intermediate are reacted to obtain the warm-mixing agent. The epoxy asphalt mixture has good Marshall stabilization degree, rut resistance and water damage resistance capabilities.
Owner:CHINA PETROLEUM & CHEM CORP +1

A kind of hot-melt marking paint and preparation method thereof

The invention relates to the technical field of traffic paint and in particular relates to hot-melt traffic paint and a preparation method thereof. According to the paint, multiple functional aids areselected to be combined to be used, the wear resistance, cracking resistance, corrosion resistance and antifouling property of the paint are improved. The primer paint can be well combined with the ground, so that pavement micro-pores are closed, the variation of the pavement and traffic line deformation under high-temperature or high-pressure conditions can be balanced, cracking even drop of thetraffic line caused by the variation of the deformation is reduced, and the mind-set of improving the cracking resistance, drop and other inner performances of the traffic line by adjusting the components and doses of various aids in the paint only in the traditional paint is broken; coloring pigments and auxiliary luminous materials are added into intermediate paint layer to serve as a traffic sign luminous layer and are combined with the surface paint to be used; glass beads are added into the surface paint, so that the reflective refraction of the coating is improved. Due to rare-earth high polymer photoluminescence materials and nano fluorescent particles in the intermediate layer and the surface layer, the visibility of the traffic line is obviously improved.
Owner:WELL ROAD MACHINERY CO LTD

Preparation method of low-cost anti-segregation anti-aging modified asphalt

The invention discloses a preparation method of low-cost anti-segregation anti-aging modified asphalt, which adopts styrene butadiene styrene triblock copolymer (SBS), polyphosphoric acid (PPA), a stabilizer, rubber oil and other materials to modify 90 # A-grade road petroleum asphalt, thereby the low-cost anti-segregation anti-aging composite modified asphalt is prepared, and various performanceindexes of the 90 # grade-A road petroleum asphalt should meet the specification requirements. The use amount of the SBS is more than 2.5%; wherein the dosage of the stabilizer is more than 0.05%, andthe dosage of the rubber oil is more than 1.5%. The SBS modifier is added into the 90 # asphalt, stirring is carried out for 30 minutes by adopting a constant-temperature stirrer, the stabilizer andthe rubber oil are doped into the swollen modified asphalt, shearing is performed for 40 minutes by adopting a high-speed shearing machine, the condition that a large number of bubbles are generated on the surface of the asphalt in the shearing process can be observed and the shearing rate basically does not change suddenly, and the shearing is completed. According to the invention, the use amountof SBS can be reduced by about 0.6%-0.8%, and the cost can be reduced by at least 81 yuan / ton.
Owner:黄伟

Semi-flexible functional combined structure recovery layer applied to asphalt pavement maintenance

The invention discloses a semi-flexible functional combined structure recovery layer applied to asphalt pavement maintenance. The rear semi-flexible functional combined structure recovery layer of themilled original upper middle surface layer sequentially comprises an SBS modified asphalt bonding layer, a polymer modified cement paste poured macroporous asphalt mixture semi-flexible middle surface layer, a synchronous broken stone sealing layer and an ultrathin wearing layer from bottom to top, wherein the polymer modified cement paste poured macroporous asphalt mixture semi-flexible middle surface layer has thickness of 7-9 cm, the material is specifically polymer modified cement paste poured macroporous asphalt mixture,, the synchronous broken stone sealing layer is composed of SBS modified asphalt and limestone with the single particle size of 7.2-9.5 mm, thickness of the ultrathin wearing layer is 1.5-2.5 cm, the ultra-thin wearing layer is made of a densely-prepared SBS modifiedasphalt mixture, and total thickness of the semi-flexible function combination structure recovery layer is the same as the milling thickness. The rear semi-flexible functional combined structure recovery layer can be applied to the field of asphalt pavement maintenance such as asphalt pavement structural damage repair and heavy-load traffic pavement function improvement.
Owner:GUANGXI JINMENG ENG

High-viscosity and high-elastic modified asphalt produced from Patuosi crude oil straight-run asphalt and preparation method thereof

The invention relates to a high-viscosity and high-elastic modified asphalt produced from Patuosi crude oil straight-run asphalt and a preparation method thereof. The high-viscosity and high-elastic modified asphalt comprises the raw materials: 85-90 parts by mass of matrix asphalt, 5-10 parts by mass of an SBS modifying agent, 1-2 parts by mass of extract oil, 2-4 parts by mass of a ductility improver, and 0.1-0.3 part by mass of a stabilizer; the high-viscosity and high-elastic modified asphalt has low cost, has the 60 DEG C viscosity of greater than 100000 Pa.s, is an excellent-performance asphalt binding material, can be applied to bridge deck pavement, drainage pavements and water permeable pavements, can effectively improve the durability of an asphalt mixture, and fully meets the use requirements of a drainage asphalt mixture; the blended asphalt mixture has excellent moisture damage resistance, rut resistance and flying resistance.
Owner:FOSHAN GAOFU PETROCHINA FUEL ASPHALT

PG82-22 grade modified asphalt and production method thereof

The invention discloses PG82-22 grade modified asphalt and a production method thereof. The modified asphalt comprises the following components in parts by weight: 100 parts of road petroleum asphalt, 4.0-6.0 parts of an SBS modifier, 0-3.0 parts of rubber oil, 0-3.0 parts of a PG reinforcing agent and 0.1-0.5 part of a stabilizer, wherein the road petroleum asphalt is straight-run asphalt of which the needle penetration at 25 DEG C is 60-800.1 mm and the ductility at 10 DEG C is greater than 100cm; specifically, at least one of imported Korean double dragon 70 # asphalt, Korean SK70 # asphalt and Korean GS70 # asphalt is selected and mixed with at least one of domestic asphalt Dalian Xitai 70 #, Zhenhai 70 #, Shandong leap city 70 #, Shandong Jingbo 70 # and Shandong Hai right 70 # in proportion; the PG reinforcing agent is a new material HW type product of Wenchang in Jiangsu. By adding the PG reinforcing agent, the high-temperature PG performance of the asphalt is improved, the viscosity of the asphalt is improved, the compatibility among the components is good, separation and layering are avoided, and the asphalt has excellent rutting resistance and ageing resistance and has good practicability and economical efficiency.
Owner:江苏亿虎沥青材料有限公司

A kind of high modulus oil corrosion resistant asphalt mixture and preparation method thereof

The invention relates to a high-modulus anti-oil-corrosion asphalt mixed material. The asphalt mixed material contains the following components: an aggregate with a particle size of 10mm-15mm, an aggregate with a particle size of 5mm-10mm, an aggregate with a particle size of 3mm-5mm, an aggregate with a particle size of 0-3mm, mineral powder with a particle size of 0-0.15mm, glass fiber, a high-modulus modifying agent, an anti-oil-corrosion agent and matrix asphalt. The invention simultaneously provides a preparation method of the high-modulus anti-oil-corrosion asphalt mixed material. The high-modulus anti-oil-corrosion asphalt mixed material has a relatively good anti-oil-corrosion effect and simultaneously has relatively high modulus, and a production process is simple; and the anti-oil-corrosion agent is used by virtue of a direct feeding method, and asphalt modifying equipment and other equipment are not additionally required in the construction, so that the construction is relatively convenient.
Owner:CHECC HIGHWAY MAINTENANCE & TEST TECH CO LTD +2

Warm-mix epoxy asphalt, mixture containing it and preparation method thereof

The invention discloses warm mixed epoxy asphalt. The product comprises a warm mixed asphalt, an epoxy resin composition and a curing agent. The warm mixed asphalt comprises a warm mixing agent and matrix asphalt. The warm mixing agent is prepared by performing a sweating process by taking a byproduct polyethylene wax as a raw material. In the sweating process, oil soluble organic matters capable of decomposed to generate gas are pre-added into the byproduct polyethylene wax raw material, and micro-bubbles are formed in a wax layer by means of gas generated by the byproduct polyethylene wax which is heated, so that a liquid component is quickly discharged and separated; meanwhile, in the sweating process, the liquid component is carried out through the wax layer by means of the air flow to separate the solid component from the liquid component in a forced manner, so that the low molecular weight components in the raw material are removed more effectively. The warm mixing agent used in the product not only can play a warm mixing role on the asphalt, but also can improve the thermal stability of the asphalt, improve the anti-thermal aging property, reduce the fusing temperature of the asphalt and the viscosity at the temperature, and reduce the generation amount of harmful gas.
Owner:CHINA PETROLEUM & CHEM CORP +1

A kind of warm mix asphalt mixture and preparation method thereof

The invention discloses a preparation technology of a warm mix asphalt mixture. The warm mix asphalt mixture comprises 88-93 parts of mineral aggregate, 6-10 parts of modified warm mix asphalt and 1-2parts of fibers, wherein the modified warm mix asphalt comprises the following ingredients in parts by weight: 66-76 parts of matrix asphalt, 7.5-10 parts of rubber cracking oil, 6-8 parts of plasticcracking wax, 6-7 parts of alkene oil, 2-4 parts of a polymer, 2-4 parts of fatty acid and 0.5-1 part of an additive. The preparation technology comprises the steps of feeding the mineral aggregate heated to 120-140 DEG C into a blending cylinder, adding heated asphalt at 105-125 DEG C and a warm mix asphalt modifier, performing stirring 2-4 min, feeding the fibers, and performing blending for 0.5-1 min to form the warm mix asphalt mixture. The performance, such as water damage resistance, rut resistance and fatigue resistance, of the warm mix asphalt mixture are improved; when the warm mix asphalt mixture is applied to road construction, a service life of a road is effectively prolonged; and the preparation technology is simple and low in cost, has great economic and social benefits andmeets the characteristics of green ecology and sustainable development.
Owner:内蒙古高速公路集团有限责任公司

Warm-mix asphalt additive and preparation method thereof

The invention relates to a warm-mix asphalt additive and a preparation method thereof. The additive comprises the following components in percentage by weight: 87 to 98 percent of chemical modification latex, 0.5 to 12 percent of lubricative and peeling resistant cation surfactant and 0.1 to 2.0 percent of acid. The method comprises the following steps of: heating the chemical modification latex to the temperature of between 40 and 80 DEG C with stirring, and dripping 0.1 to 0.5 percent of acid slowly; adding the lubricative and peeling resistant cation surfactant, stirring fully, and dispersing uniformly; and continuing to drip 0.1 to 1.5 percent of acid slowly, stirring uniformly, keeping the temperature of between 40 and 80 DEG C and storing for later use. By the warm-mix asphalt additive and the preparation method, the viscosity of asphalt binders during mixing can be reduced effectively, the reduction performance of asphalt cements and adhesivity between the asphalt cements and aggregates can be improved, the water damage resistance and durability of warm-mix asphalt mixtures can be improved, the tensile strength of asphalt can be improved, and the rutting resistance, fatigueresistance and low temperature resistance of the warm-mix asphalt mixtures can be enhanced.
Owner:PETROCHINA CO LTD +1

Warm-mixed asphalt mixture and preparation method thereof

The invention relates to a warm-mixed asphalt mixture and a preparation method thereof. The warm-mixed asphalt mixture is mainly applied to new construction and maintenance of high-grade roads and common roads, and is particularly suitable for cities, parks, tunnels and the like with high environmentally-friendly requirements. The warm-mixed asphalt mixture mainly comprises about 92.4-96.5 percent by weight of mineral, about 3.4-7.5 percent by weight of asphalt cement and 0.05-1.0 percent by weight of chemical modified adhesive cement. The preparation method comprises the following steps of: simultaneously pumping the chemical modified adhesive cement and the hot asphalt cement to the spraying port of a foam generator, fully mixing to generate a foam-containing hot asphalt mixture, spraying the foam-containing hot asphalt mixture into a mixing pan, and further mixing the foam-containing hot asphalt mixture and the hot mineral to form the warm-mixed asphalt mixture. The chemical modified adhesive cement can effectively reduce the mixing, spreading and rolling temperature of the asphalt mixture, and solves the problems of environmental pollution, high energy consumption, asphalt ageing regression and the like. By selecting high-concentration cationic chemical modified latex as a matrix stock of the chemical modified adhesive cement and simultaneously matching a proper proportionof cationic surfactant with lubricating effect and peeling resistance, the influence of the conventional warm-mixed asphalt additive on poor reducing performance and poor adhesive performance of the asphalt cement is solved, and the properties of the warm-mixed asphalt mixture such as water damage resistance, rutting resistance, fatigue resistance, low temperature resistance and the like are improved.
Owner:PETROCHINA CO LTD

Drainage pavement composite structure suitable for heavy traffic

The invention belongs to the field of road and bridge engineering, and particularly relates to a drainage pavement composite structure suitable for heavy traffic, the drainage pavement composite structure comprises an upper surface layer, a sealing layer, a middle surface layer, an anti-cracking bonding layer, a lower surface layer, a bonding layer and a base layer from top to bottom, the upper surface layer is a high-viscosity composite modified OGFC-13 open-graded asphalt mixture layer, and the thickness of the upper surface layer is 30-50 mm; the middle surface layer is a semi-flexible bearing layer with the nominal maximum particle size of 13.2 mm, and the thickness of the middle surface layer is 30-50 mm; and the lower surface layer is a high-viscosity composite modified discontinuous semi-open graded asphalt mixture layer with the nominal maximum particle size of 19mm or 26.5 mm, and the thickness of the lower surface layer is 50mm-80mm. The drainage pavement composite structure meets the use requirements of heavy traffic on the basis of having the advantages of the drainage pavement.
Owner:SHANGHAI PUDONG ROAD & BRIDGE GRP CO LTD

A kind of asphalt road laying method

The invention discloses an asphalt road paving method, and belongs to the field of road paving methods. The asphalt road paving method disclosed by the invention comprises five steps: a first step of performing measurement and alignment, comprising the steps of re-measuring a guiding line, a center line and a benchmark, performing cross section inspection and supplementary measurement, performing staking out in construction before the start of the construction, staking out specific locations such as the edges of a roadbed, slope openings, slope toes, side ditch berms and soil pits, indicating contours of the specific locations, clearing away trees, weeds, shrubs and the like in the range of a route land, and digging the roadbed; and other four steps. The asphalt road paving method disclosed by the invention has the characteristics of being high in flatness, free from situations such as insufficient local degree of compaction and serious temperature segregation, good in road surface temperature sensing performance, good in elasticity and aging resistance, not easy to melt and flow at high temperature, and good in toughness and not easy to break at low temperature, the use requirements of high-level roads can be met, and besides, the high temperature of a road surface can be fully utilized for solar power generation.
Owner:广东粤路勘察设计有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products