44results about How to "Excellent final dyeing effect" patented technology

Dyeing method of wool fiber top

InactiveCN106337299AExcellent light fastnessGood dyeing uniformityDyeing processDimethyl formamideN-methyldiethanolamine
The invention discloses a dyeing method of wool fiber top, comprising the following steps: 1) successively adding tristyrylphenol polyoxyelhylene ether sulfonate, acryloyloxyethyltrimethyl ammonium chloride, polyvinylpyrrolidone, dimethyl formamide and vegetable dye into a dye vat and successively pouring deionized water, uniformly stirring and heating to 45 DEG C; 2) successively pouring N-methyldiethanolamine, linear alklybezene sulfonates, magnesium sulfate and nitrilotriacetic acid, continuously stirring until the materials are fully and uniformly mixed, and heating to 60 DEG C; 3) immersing top into the dye vat for 50 min; 4) drying the immersed top at 85 DEG C; 5) immersing the dried top in clear water and rinsing for 50 min; and 6) taking the rinsed top out of the clear water and naturally airing. The top dyed by the above method has excellent color fastness and has good dyeing uniformity and has no dyeing defect.
Owner:常熟市新华源有色毛条厂

Dyeing method for textile fabric

InactiveCN106320010AExcellent color fastness to chlorine bleachingExcellent color fastness to washingDyeing processMelamineClean water
The invention discloses a dyeing method for textile fabric. The method comprises the steps of 1) Adding t-Butyl perbenzoate, 1 glycine, hydroxypropyl methylcellulose, propenoic acid ester and vegetable dyes in the deionized water in sequence, mixing even and heating to 55oC; 2) Adding hydroxycarboxylic acid, iso-tridecanol polyoxyethylene ether, dimethylamine and 0.7 parts of hexakis(methoxymethyl)melamine and mixing even, heating to 65oC; 3) Soaking the fabric in the dye vat for 25min; 4) Drying the soaked fabric at 80oC; 5) Soaking the dried fabric in clean water and rinsing for 25min; 6) Getting out the rinsed fabric and making it dry naturally. The dyed fabric is excellent in color fastness and good in dyeing uniformity, free of color tone.
Owner:常熟市华谊织造有限公司

Method for dyeing PV pile fabric

The invention discloses a method for dyeing a PV pile fabric. The method comprises the following steps: (1) sequentially adding tea polyphenols, diethylenetriamine, ethylene glycol, a maleate-acrylate copolymer and vegetable dyes into a dye vat, successively adding deionized water into the dye vat, uniformly stirring, and heating the dye vat to the temperature of 45 DEG C; (2) then, sequentially adding ethylenediamine, iso-tridecanol polyoxyethylene ether, an N-vinyl pyrrolidone / acrylamide copolymer and 2-acrylic acid amide-2-methylpropanesulfonic acid into the dye vat, continuing stirring until the mixture is uniformly mixed thoroughly, and heating the dye vat to the temperature of 60 DEG C; (3) soaking the fabric in the dye vat for 45 minutes; (4) baking the soaked fabric at the temperature of 85 DEG C; (5) submerging the baked fabric in clean water, and rinsing for 45 minutes; (6) taking out the rinsed fabric, and naturally drying the fabric in the air. According to the method, the dyed fabric has excellent color fastness, is good in dyeing uniformity and is free of uneven dyeing.
Owner:常熟市绮丽家纺有限公司

Shu velveteen fabric dyeing method

The invention discloses a Shu velveteen fabric dyeing method. The Shu velveteen fabric dyeing method comprises the following steps: 1) polyethylene glycol fatty acid ester, borax, polyacrylic acid, dimethylamine and a vegetable dye are added to deionized water in a dye vat sequentially, and the materials are stirred uniformly and heated to 45 DEG C; 2) then alkyl polyglucoside, sodium alkyl ester sulfosuccinate, n-butyl acrylate and titanium dioxide are fed sequentially, and the materials are stirred continuously until the materials are mixed sufficiently and uniformly and are heated to 60 DEG C; 3) the fabric is soaked in the dye vat for 40 min; 4) the soaked fabric is dried at 85 DEG C; 5) the dried fabric is soaked in clear water and rinsed for 40 min; 6) the rinsed fabric is taken out and aired naturally. The fabric dyed with the method has excellent color fastness and dyeing evenness and is free of colored spots.
Owner:SUZHOU YUHUA BUSINESS MANAGEMENT CO LTD

Silk fabric dyeing method

The invention discloses a silk fabric dyeing method which includes the steps: 1) sequentially adding titanium dioxide, beta-aminopropionic acid, N-methyl pyrrolidone, sodium silicate and plant dyestuff into a dye vat, sequentially adding raw materials into deionized water, uniformly stirring the raw materials and heating the raw materials to reach 55 DEG C; 2) sequentially adding chitosan, secondary alkane sulphonate sodium, urea and dibutyl phthalate, continuing stirring until sufficiently and uniformly mixing the raw materials, and heating the raw materials to reach 65 DEG C; 3) soaking a fabric in the dye vat for 25 minutes; 4) drying the soaked fabric at the temperature of 80 DEG C; 5) soaking the dried fabric in clear water and rinsing the fabric for 25 minutes; 6) taking out the rinsed fabric and naturally airing the fabric. The dyed fabric has excellent color fastness and is good in dyeing uniformity and free from dyeing defects.
Owner:常熟市华谊织造有限公司

Dyeing method for garment fabric

InactiveCN106351031AExcellent color fastness to chlorine bleachingGood dyeing uniformityDyeing processGum arabicDyeing
The invention discloses a dyeing method for a garment fabric. The dyeing method comprises the following steps: 1) sequentially adding aluminium oxide powder, acroleic acid, gum arabic powder, polyurethane and a wood dye into deionized water in a dye vat, uniformly stirring all the raw materials, and heating the mixture to 55 DEG C; 2) then sequentially feeding fumaric acid, maleic acid acrylic polymer, aqueous ammonia and dibutyltin dilaurate, and continuously stirring until all the ingredients are uniformly mixed, and heating the mixture to 65 DEG C; 3) soaking the fabric in the dye vat for 25 minutes; 4) drying the soaked fabric at a temperature of 80 DEG C; 5) immerging the dried fabric in clear water, and rinsing the fabric for 25 minutes; and 6) taking out the rinsed fabric, and naturally airing the fabric. The fabric dyed by the dyeing method has excellent color fastness, and is good in dyeing uniformity and free from dyeing defect.
Owner:常熟市华谊织造有限公司

Dyeing method for stretching wool top

InactiveCN106149406AExcellent light fastnessGood dyeing uniformityDyeing processAmmonium sulfateWool
The invention discloses a dyeing method for a stretching wool top. The dyeing method comprises the following steps: 1) adding sodium ethylenediamine tetramethylene, fatty alcohol-polyoxyethylene ether, hydroxyethyl cellulose, tristyrylphenol polyoxyethylene ether ammonium sulfate and vegetable dyes into a dye vat in turn, adding deionized water, uniformly stirring and heating to 45 DEG C; 2) adding diallyl ammonium salt, sodium sulfamate, aluminum oxide powder and crylic acid in sequence, continuing to stir till uniformly mixing, and heating to 60 DEG C; 3) soaking the wool top into the dye vat for 50 minutes; 4) drying the soaked wool top at 85 DEG C; 5) soaking the dry wool top in clean water and washing for 50 minutes; 6) taking the washed wool top out and then naturally airing. The dyed wool top provided by the invention has excellent color fastness, high leveling of dyeing and no dyeing defect.
Owner:常熟市新华源有色毛条厂

Pine needle fleece fabric dyeing method

The invention discloses a pine needle fleece fabric dyeing method. The pine needle fleece fabric dyeing method comprises the following steps: 1) ethylene carbonate, glacial acetic acid, hydroxypropyl cellulose, triethylenetetramine and a vegetable dye are added to deionized water in a dye vat sequentially, and the materials are stirred uniformly and heated to 45 DEG C; 2) then sodium glycinate, sodium sulfamate, acryloyloxyethyltrimethyl ammonium chloride and polyurethane are fed sequentially, and the materials are stirred continuously until the materials are mixed sufficiently and uniformly and are heated to 60 DEG C; 3) the fabric is soaked in the dye vat for 40 min; 4) the soaked fabric is dried at 85 DEG C; 5) the dried fabric is soaked in clear water and rinsed for 40 min; 6) the rinsed fabric is taken out and aired naturally. The fabric dyed with the method has excellent color fastness and dyeing evenness and is free of colored spots.
Owner:SUZHOU YUHUA BUSINESS MANAGEMENT CO LTD

Dyeing method for corduroy fabric

The invention discloses a dyeing method for a corduroy fabric. The dyeing method comprises the following steps: 1) adding dicyandiamide, sodium ethylene diamine tetracetate, glycol, ethylene carbonate and vegetable dye into a dye vat in turn, adding deionized water, uniformly stirring and heating to 55 DEG C; 2) adding sodium hexametaphosphate, sodium dodecyl sulfate, o-phthalimide and polyethylene glycol in turn, stirring till uniformly mixing, and then heating to 65 DEG C; 3) soaking the fabric into the dye vat for 30 minutes; 4) drying the fabric after being soaked at 80 DEG C; 5) soaking the fabric after being dried into clean water and washing for 30 minutes; 6) taking out the fabric after being washed and then naturally airing. According to the invention, the fabric after being dyed has excellent color fastness, high leveling of dyeing and no dyeing defect.
Owner:常熟市通惠织造有限公司

Dyeing method of flannel fabric

The invention discloses a dyeing method of flannel fabric. The dyeing method comprises the following steps: 1) sequentially adding sodium sulfate, ammonia water, sodium hexametaphosphate, hydantoin and vegetable dye into deionized water, uniformly stirring, and heating to 45 DEG C; 2) then sequentially putting methylallylamine hydrochloride, sodium alkyl benzene sulfonate, triethanolamine and a monomer containing tertiary amino, further stirring until the substances are fully and uniformly mixed, and heating to 60 DEG C; 3) soaking the fabric in a dyeing vessel for 45 minutes; 4) drying the soaked fabric at the temperature of 85 DEG C; 5) immersing the dried fabric into clean water and rinsing for 45 minutes; and 6) taking out the rinsed fabric, and naturally airing. The dyed fabric has excellent colour fastness, dyeing uniformity is good, and no dyeing defect is produced.
Owner:常熟市绮丽家纺有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products