A dyeing method, the technique of relaxing cotton velvet, which is applied in the field of dyeing cotton velvet fabrics, can solve the problems of poor dyeing uniformity, low color fastness of dyed fabrics, easy to produce color flowers, etc., and achieve excellent color fastness to washing , Good dyeing uniformity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0039] The dyeing method of Shu cotton wool fabric, comprises the steps:
[0040] 1) Add 1 to 2 parts by weight of polyethylene glycol fatty acid ester, 0.3 parts by weight of borax, 2.6 parts by weight of polyacrylic acid, 1.1 parts by weight of dimethylamine, and 20 parts by weight of vegetable dyes into the dye vat in turn, and add 100 parts by weight of deionized water , stir evenly, and heat to 45°C;
[0041] 2) Add 1.5 parts by weight of alkyl polyglucoside, 0.9 parts by weight of sodium alkyl sulfosuccinate, 1.9 parts by weight of n-butyl acrylate, and 0.5 parts by weight of titanium dioxide, and continue stirring until fully mixed and heated to 60°C;
[0042] 3) Soak the fabric in the dye vat for 40 minutes;
[0043] 4) drying the soaked fabric at 85°C;
[0044] 5) soak the dried fabric in clean water and rinse for 40 minutes;
[0045] 6) Take out the rinsed fabric and let it dry naturally.
Embodiment 2
[0047] The dyeing method of Shu cotton wool fabric, comprises the steps:
[0048] 1) Add 1 part by weight of fatty acid polyethylene glycol ester, 0.3 part by weight of borax, 2.6 parts by weight of polyacrylic acid, 1.1 parts by weight of dimethylamine, and 20 parts by weight of vegetable dyes into 100 parts by weight of deionized water successively in the dye vat, stirring uniform, and heated to 45 ° C;
[0049] 2) Add 1.5 parts by weight of alkyl polyglucoside, 0.9 parts by weight of sodium alkyl sulfosuccinate, 1.9 parts by weight of n-butyl acrylate, and 0.5 parts by weight of titanium dioxide, and continue stirring until fully mixed and heated to 60°C;
[0050] 3) Soak the fabric in the dye vat for 40 minutes;
[0051] 4) drying the soaked fabric at 85°C;
[0052] 5) soak the dried fabric in clean water and rinse for 40 minutes;
[0053] 6) Take out the rinsed fabric and let it dry naturally.
Embodiment 3
[0055] The dyeing method of Shu cotton wool fabric, comprises the steps:
[0056] 1) Add 2 parts by weight of fatty acid polyethylene glycol ester, 0.3 parts by weight of borax, 2.6 parts by weight of polyacrylic acid, 1.1 parts by weight of dimethylamine, and 20 parts by weight of vegetable dyes into 100 parts by weight of deionized water successively in the dye vat, and stir uniform, and heated to 45 ° C;
[0057] 2) Add 1.5 parts by weight of alkyl polyglucoside, 0.9 parts by weight of sodium alkyl sulfosuccinate, 1.9 parts by weight of n-butyl acrylate, and 0.5 parts by weight of titanium dioxide, and continue stirring until fully mixed and heated to 60°C;
[0058] 3) Soak the fabric in the dye vat for 40 minutes;
[0059] 4) drying the soaked fabric at 85°C;
[0060] 5) soak the dried fabric in clean water and rinse for 40 minutes;
[0061] 6) Take out the rinsed fabric and let it dry naturally.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com