An environmentally friendly, photoinitiator technology, applied in chemical instruments and methods, inorganic chemistry, coatings, etc., can solve the problems of high viscosity, poor absorption, and eye irritation of oligomers, and achieve strong gloss and strong adsorption Performance, effect of preventing water mist phenomenon
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0041] An environment-friendly moisture-proof UV varnish, the environment-friendly moisture-proof UV varnish comprises the following components in parts by weight: 30 parts of polyurethane-acrylate prepolymer, 5 parts of photoinitiator, 0.1 part of tribasic lead sulfate, ethyl acetate 0.1 part of glycol monobutyl ether, 0.1 part of polyoxyethylene polyoxypropylene pentaerythritol ether and 1 part of nano-bimetal oxide adsorption material; polyurethane-acrylate prepolymer is composed of toluene diisocyanate, polyether diol, ethylene glycol , dimethylol propionic acid, acetone, hydroxyethyl methacrylate, hydroquinone and triethylamine; nano-bimetallic oxide adsorption material is made of magnesium nitrate, aluminum nitrate, N,N-dimethyl Prepared from acetamide, 1-butyl-3-methylimidazolium hexafluoroantimonate, ammonia water and deionized water; photoinitiators are 2-hydroxy-2-methyl-1-phenylacetone and 2,4 , A mixture of ethyl 6-trimethylbenzoyl phenylphosphonate in a weight rat...
Embodiment 2
[0051] An environment-friendly and moisture-proof UV varnish, which comprises the following components in parts by weight: 35 parts of polyurethane-acrylate prepolymer, 6 parts of photoinitiator, 0.2 part of dibasic lead phosphite, 0.15 part of acrylic copolymer, 0.2 part of polyoxyethylene polyoxypropanolamine ether and 2 parts of nano-bimetal oxide adsorption material; polyurethane-acrylate prepolymer is composed of isophorone diisocyanate, perfluoropolyether diol , 1,3-propanediol, dimethylol propionic acid, acetone, hydroxyethyl methacrylate, hydroquinone and triethylamine; the environmental protection moisture-proof UV varnish also includes 1-5 parts by weight The nano-bimetal oxide adsorption material is composed of magnesium chloride, aluminum chloride, N,N-dimethylacetamide, 1-butyl-3-methylimidazole hexafluoroantimonate, ammonia water It is prepared from deionized water; the photoinitiator is 2-hydroxy-2-methyl-1-phenylacetone and 2,4,6-trimethylbenzoyl phenylphosphon...
Embodiment 3
[0061] An environment-friendly and moisture-proof UV varnish, which comprises the following components in parts by weight: 40 parts of polyurethane-acrylate prepolymers, 7.5 parts of photoinitiators, and 0.3 parts of tribasic lead maleate , 0.2 parts of polydimethylsiloxane, 0.3 parts of polyoxypropylene glycerol ether and 3 parts of nano-bimetal oxide adsorption material; polyurethane-acrylate prepolymer is composed of diphenylmethane diisocyanate, aliphatic polyester binary It is prepared from alcohol, 1,2-butanediol, dimethylolpropionic acid, acetone, hydroxyethyl methacrylate, hydroquinone and triethylamine; the environmental protection moisture-proof UV varnish also includes 1-5 The nanometer double metal oxide adsorption material in parts by weight, the nanometer double metal oxide adsorption material is composed of magnesium sulfate, aluminum sulfate, N,N-dimethylacetamide, 1-butyl-3-methylimidazole hexafluoroantimonic acid salt, ammonia and deionized water; photoinitia...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com