The invention relates to a
geopolymer chemically-bonded
ceramic tile and a preparation method thereof. The
geopolymer chemically-bonded
ceramic tile is prepared from
solid wastes like
fly ash, filtered steel and
copper slag, and industrial-grade chemical raw materials. The unburned
ceramic tile is prepared from, by
mass, 60 to 75% of the
solid wastes, 19 to 38% of a liquid activator, 1 to 3% of a base-material additive and 1 to 3% of a compound liquid additive by procedures like mixing, sieving and granulating. Due to implementation of a firing-free process, energy conversation and consumption reduction can be realized;
pollution is reduced; meanwhile, performances of the
geopolymer chemically-bonded ceramic tile can reach national standards of fired
ceramic tiles. The geopolymer ceramic tile does not need to introduce calcined kaolin, and after 12 to 48 hours of easy and practicable special maintenance, a ceramic bonded three-dimensional network body is rapidly formed, so the ceramic tile reaches and is superior in a part of performances to the 60-day-age level of similar geopolymer materials; limited mineral resources are not consumed; and
energy consumption of
calcination is avoided. The geopolymer chemically-bonded ceramic tile provided by the invention can change wastes into treasures, significantly saves energy and reduces consumption, can be used as a novel
building material and has extensive application prospects.