The invention provides a method for
machining a shock-resistant
assembly self-locking type half grouting sleeve and a method for
machining a concrete member. The method for
machining the shock-resistant
assembly self-locking type half grouting sleeve comprises the steps that (1) the grouting sleeve is machined in a
casting mode and integrally formed, one end of the grouting sleeve is subjected toinner thread treatment, and a plurality of mounting holes are formed in a sleeve body for standby application; (2) one end of a steel
pipe transition section is subjected to outer thread treatment forstandby application; (3) firstly, a plurality of longitudinal guiding steel bars and a plurality of circumferential fixing steel rings are welded to form cylindrical keels, then a plurality of inclined steel branches are welded on a plurality of annular sections of the keels in emissive and inclined
modes to form inner barbs and outer barbs for standby application; and (4)
assembly is conducted.All parts of the grouting sleeve are machined and manufactured correspondingly and then assembled,
mass production is achieved, and the quality of all the parts is easy to control; connection of the grouting sleeve and the steel
pipe transition section is operated by machines in a factory, the threaded connection quality is easy to control, a first to-be-connected
steel bar and the steel
pipe transition section directly adopt the rolling mode, thus the connecting working procedure is simple, and the lengths of the
steel bar parts inserted into the sleeve are easy to control; and a self-lockingtype steel skeleton is adopted, so that pulling preventing is achieved.