A monolithic column, inorganic technology, applied in the field of detection, can solve the problems of reduced stability and mechanical properties, intolerant of organic solvent swelling, poor thermal stability, etc., to achieve enhanced mechanical properties, good thermal stability, good porosity. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment Construction
[0034] In parts by weight, weigh 5~10 parts of copper perchlorate, 10~20 parts of melamine, 1~2 parts of citric acid, 20~40 parts of N,N-dimethylformamide, and add the copper perchlorate , Melamine and citric acid are added to N,N-dimethylformamide, stir and mix at 180~200r / min for 10~12min at room temperature, and let stand for 20~24h to obtain a copper ion mixture. Place the copper ion mixture In an ultrasonic dispersing machine, ultrasonically vibrate for 15-20min under the condition of 400~500W to obtain copper metal organic gel; then weigh 20~30 parts of ethyl orthosilicate and 8~12 parts by weight. Anhydrous ethanol, 16~24 parts of 25% by mass ammonia water, 20~30 parts of deionized water, add anhydrous ethanol and ammonia to deionized water, and stir at 120~160r / min for 10~12min at room temperature to obtain alcohol Ammonia hydrolysis solution, add 1 / 3 ethyl orthosilicate to 1 / 3 alcohol ammonia hydrolysis solution, stir at 240~280r / min for 30~40min under refrigerated con...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com