Super-hydrophobic heat-resistant coating for aluminum alloy and preparation method of super-hydrophobic heat-resistant coating
A technology of super-hydrophobic coating and heat-resistant coating, applied in metal material coating process, coating, device for coating liquid on the surface, etc. It is difficult to stabilize production and other problems, and achieve the effect of preventing thermal migration and improving heat resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0031] A method for preparing a superhydrophobic heat-resistant coating for an aluminum alloy, the method for preparing a superhydrophobic heat-resistant coating for an aluminum alloy mainly includes the following preparation steps:
[0032] (1) Spraying pretreatment: Polish the aluminum alloy with 220-mesh sandpaper for 5 minutes, soak it in an alkali cleaning solution twice the quality of the aluminum alloy, and the mass ratio of sodium carbonate, sodium silicate, sodium phosphate and deionized water in the alkali cleaning solution is 1:0.5:1:18, after soaking at 70°C for 8 minutes, rinse with deionized water for 3 minutes to obtain a pretreated aluminum alloy; Mix water at a mass ratio of 1:122, add glacial acetic acid until the pH of the solution is 4, let stand for hydrolysis for 24 hours, and make a silane solution; place the pretreated aluminum alloy on a glass plate, and spray a silane solution 0.3 times the mass of the pretreated aluminum alloy , and then cured at 90°...
Embodiment 2
[0038] A method for preparing a superhydrophobic heat-resistant coating for an aluminum alloy, the method for preparing a superhydrophobic heat-resistant coating for an aluminum alloy mainly includes the following preparation steps:
[0039] (1) Spraying pretreatment: Polish the aluminum alloy with 240-mesh sandpaper for 3 minutes, soak it in an alkali cleaning solution 2.14 times the quality of the aluminum alloy, and the mass ratio of sodium carbonate, sodium silicate, sodium phosphate and deionized water in the alkali cleaning solution is 1:0.5:1:18, after soaking at 75°C for 6 minutes, rinse with deionized water for 5 minutes to obtain a pretreated aluminum alloy; Mix water at a mass ratio of 1:123, add glacial acetic acid until the pH of the solution is 4.5, let stand for hydrolysis for 26 hours, and make a silane solution; place the pretreated aluminum alloy on a glass plate, and spray a silane solution that is 0.4 times the mass of the pretreated aluminum alloy , and th...
Embodiment 3
[0045] A method for preparing a superhydrophobic heat-resistant coating for an aluminum alloy, the method for preparing a superhydrophobic heat-resistant coating for an aluminum alloy mainly includes the following preparation steps:
[0046] (1) Spraying pretreatment: Polish the aluminum alloy with 240-mesh sandpaper for 5 minutes, soak it in an alkali cleaning solution that is 3 times the quality of the aluminum alloy, and the mass ratio of sodium carbonate, sodium silicate, sodium phosphate and deionized water in the alkali cleaning solution is 1:0.5:1:18, after soaking at 80°C for 5 minutes, rinse with deionized water for 7 minutes to obtain a pretreated aluminum alloy; Mix water at a mass ratio of 1:124, add glacial acetic acid until the pH of the solution is 5, let stand for hydrolysis for 28 hours, and make a silane solution; place the pretreated aluminum alloy on a glass plate, and spray a silane solution 0.5 times the mass of the pretreated aluminum alloy , and then cu...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com