A kind of preparation method of magnetic sewage treatment agent
A sewage treatment agent and magnetic technology, applied in water/sewage treatment, magnetic field/electric field water/sewage treatment, light water/sewage treatment, etc. Ideal and other issues, to achieve the effect of improving contact probability, low cost, and firm load
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] The chitosan that takes weight-average molecular weight is 18kDa is dissolved in the aqueous formic acid solution of 98wt%, adds DMSO dilution, then adds the polyethylene glycol that the weight-average molecular weight of chitosan equimolarity is 2kDa, continues to stir 20 minutes, Add 37wt% formaldehyde solution, stir for 1 h, add NaOH to adjust the pH value to 13, wash with absolute ethanol, and freeze-dry to obtain polyethylene glycol chitosan grafts.
[0026] Weigh iron ferric oxide nano-magnetic powder, add it into pure water, and disperse it with ultrasonic probe for 20 minutes for the first time to obtain the dispersion liquid; Dispersion agent-stabilized iron ferric oxide nano-magnetic powder dispersion; under water-bath ultrasonic conditions, add polyethylene glycol chitosan graft aqueous solution drop by drop to the water-bath ultrasonic 5min, obtain coated magnetic nanoparticle; Add soluble molybdate in organic solvent, stir and mix, obtain molybdate solution...
Embodiment 2
[0028] The preparation method of polyethylene glycol chitosan graft is identical with embodiment 1.
[0029] Weigh iron ferric oxide nano-magnetic powder, add it into pure water, and disperse with ultrasonic probe for 40 minutes for the first time to obtain a dispersion liquid; weigh the dispersant and dissolve it in absolute ethanol, add the above dispersion liquid, and ultrasonically disperse with a second probe for 15 min to obtain a Dispersion agent-stabilized iron ferric oxide nano-magnetic powder dispersion; under water-bath ultrasonic conditions, add polyethylene glycol chitosan graft aqueous solution drop by drop to the water-bath ultrasonic 10min, obtain coating magnetic nanoparticle; Add soluble molybdate in organic solvent, stir and mix, obtain molybdate solution; Add bismuth nitrate in organic solvent, stir and mix, obtain bismuth nitrate solution; Coating magnetic nanoparticle Add it into the bismuth nitrate solution and mix it for 5 hours, then add the molybdate ...
Embodiment 3
[0031] The preparation method of polyethylene glycol chitosan graft is identical with embodiment 1.
[0032] Weigh iron ferric oxide nano-magnetic powder, add it into pure water, and disperse with ultrasonic probe for 30 minutes for the first time to obtain a dispersion liquid; weigh the dispersant and dissolve it in absolute ethanol, add the above dispersion liquid, and ultrasonically disperse with a second probe for 13 min to obtain a Dispersion agent-stabilized iron ferric oxide nano-magnetic powder dispersion; under water-bath ultrasonic conditions, add polyethylene glycol chitosan graft aqueous solution drop by drop to the water-bath ultrasonic 8min, obtain coating magnetic nanoparticle; Add soluble molybdate in organic solvent, stir and mix, obtain molybdate solution; Add bismuth nitrate in organic solvent, stir and mix, obtain bismuth nitrate solution; Coating magnetic nanoparticle Add to the bismuth nitrate solution and mix for 5 hours, then add the molybdate solution,...
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com