Clobetasol propionate molecule capturer, and preparation method and applications thereof
A technology of clobetasol propionate and traps, applied in the field of molecular traps, can solve problems such as harming human health, ignorance, and destruction of hormone balance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0035] 1. Preparation of Clobetasol Propionate Molecular Capture
[0036] (1) Graphene oxide modified polyethylene filter plate
[0037] Place 4 pieces of polyethylene filter plates (diameter 5-10mm, thickness 2-3mm) in acetonitrile for several hours, take them out, and put them in jars; take 3.6mL of graphite oxide slurry with a concentration of 11.1mg / mL and add it to 6.4 In mL N,N-dimethylformamide, ultrasonically disperse into a graphene oxide sol and transfer it to a jar, place it on an oscillator and shake it at room temperature for 60 minutes, take out the filter plate, and dry it at 50°C for 1 hour; repeat coating Six times, the graphene oxide-coated polyethylene filter plate is obtained;
[0038] (2) Preparation of silanized graphene oxide coated filter plate
[0039] Put 50mL of ethanol and 20mL of water in a beaker, add 9.0mL of ammonia water, mix well and transfer to a three-necked flask, then add 20 pieces of graphene oxide-coated polyethylene filter plates, and...
Embodiment 2
[0050] 1. Preparation of Clobetasol Propionate Molecular Capture
[0051] Steps (1), (2) are the same as in Example 1.
[0052] (3) Preparation of molecularly imprinted polymer membranes containing clobetasol propionate by surface imprinting polymerization
[0053] Put 0.94g of clobetasol propionate and 9.4mL of 3-aminopropyltriethoxysilane into a beaker containing 20mL of acetonitrile, and ultrasonicate for 3min to form a pre-polymerization solution; then add 16 pieces of silanized Graphene oxide coated filter plate, sealed and protected from light for 8 hours; add 20mL tetraethyl orthosilicate, 4mL glacial acetic acid, 40mL absolute ethanol, stir well, transfer to a three-necked flask, add a stirrer, condenser, thermometer , nitrogen deoxygenation, constant temperature reaction at 30°C for 15 hours, and a molecularly imprinted polymer film containing clobetasol propionate was formed on the surface of the silanized graphene oxide-coated filter plate;
[0054] (4) Elution of...
Embodiment 3
[0060] 1. Preparation of Clobetasol Propionate Molecular Capture
[0061] Steps (1), (2) are the same as in Example 1.
[0062] (3) Preparation of molecularly imprinted polymer membranes containing clobetasol propionate by surface imprinting polymerization
[0063] Put 1.41g of clobetasol propionate and 14.1mL of 3-aminopropyltriethoxysilane into a beaker filled with 30mL of acetonitrile, and ultrasonicate for 3min to form a pre-polymerization solution; then add 24 pieces of silanized Graphene oxide coated filter plate, sealed and protected from light for 8 hours; add 30mL tetraethyl orthosilicate, 6mL glacial acetic acid, 60mL absolute ethanol, stir evenly, transfer to a three-necked flask, add a stirrer, condenser, thermometer , nitrogen deoxygenation, constant temperature reaction at 30°C for 15 hours, and a molecularly imprinted polymer film containing clobetasol propionate was formed on the surface of the silanized graphene oxide-coated filter plate;
[0064] (4) Elutio...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com