Anti-flaming static electricity conducting organic silicon nano ceramic coating used for coal-mine gas drainage pipeline
A nano-ceramic, coal mine gas technology, applied in conductive coatings, pipeline protection, anti-corrosion coatings, etc., can solve the problems of poor anti-static, flammable, low mechanical strength of protective coatings, etc., to achieve high surface energy, improve corrosion resistance. , Outstanding effect of conducting static electricity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0030] 30 parts of pure silicone resin (purchased from Zhonghao Chenguang Chemical Research Institute), 15 parts of zinc phosphate, 10 parts of silicon carbide (particle diameter, that is, particle size 50-100nm), 25 parts of mica powder, 7 parts of graphite, organic bentonite (Purchased from Liupanshui Shenyuan Mining Co., Ltd.) 2 parts were mixed with 11 parts of solvent xylene, and ground on a sand mill for 2 hours to obtain a flame-retardant and electrostatically conductive coating.
[0031] How to use: Spray the paint on the surface of the pipe, and treat it at 300°C for 2 hours after the surface is dry to form a coating.
Embodiment 2
[0033] Mix 20 parts of pure silicone resin, 13 parts of zinc phosphate, 7 parts of aluminum oxide (particle size 50-300nm), 30 parts of talcum powder, 5 parts of graphite, 1 part of organic bentonite and 24 parts of solvent toluene. Grind on a sand mill for 2.5 hours to obtain a flame retardant and static conductive coating.
[0034] How to use: Spray the paint on the surface of the pipe, and treat it at 350°C for 40 minutes after the surface is dry to form a coating.
Embodiment 3
[0036] 40 parts of pure silicone resin, 10 parts of zinc phosphate, 5 parts of silicon dioxide (particle size 50-300nm), 10 parts of kaolin, 8 parts of conductive carbon black, fumed silica (purchased from Jining Qingyun Chemical Co., Ltd.) 3 1 part is mixed with 24 parts of solvent xylene, and ground on a pin-type sand mill for 2 hours to obtain a flame-retardant and static-conductive coating.
[0037] How to use: Spray the paint on the surface of the pipe, and treat it at 320°C for 70 minutes after the surface is dry to form a coating.
PUM
Property | Measurement | Unit |
---|---|---|
diameter | aaaaa | aaaaa |
hardness | aaaaa | aaaaa |
adhesivity | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com