Conductive titanium dioxide and preparation method
A technology of conductive titanium dioxide and titanium dioxide, applied in chemical instruments and methods, conductive materials dispersed in non-conductive inorganic materials, fibrous fillers, etc. Poor optical performance and other problems, to achieve the effect of wide application range, improved electrical conductivity, and excellent performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0044] A preparation method of conductive titanium dioxide, comprising the following steps:
[0045] S1: Take uncoated titanium dioxide and grind, wet grind, and sand grind (the particle size after wet grinding is 0.390 μm, and the particle size distribution is 1.55) (add 1% sodium hexametaphosphate to the slurry before sand grinding as Dispersant), after dilution, the concentration of the slurry is 200g / L, and the pH of the slurry is 7; the macromolecular chain PVP modifies titanium dioxide particles, and 8wt% of high molecular polymer is added to the slurry, and the temperature is kept at normal temperature. Stirring and ultrasound, the ultrasound is turned on for 10 minutes and then turned off;
[0046] S2: Adjust the pH of the slurry to 2 with dilute acid (concentration 90g / L), adjust it within 15 minutes, and homogenize for 15 minutes. Add 10% aniline monomer to the titanium dioxide slurry, stir and homogenize at room temperature for 6 hours, and then add the initiator a...
Embodiment 2
[0049] A preparation method of conductive titanium dioxide, comprising the following steps:
[0050] S1 Uncoated titanium dioxide is pulverized, wet-milled, sand-milled (add 1% sodium hexametaphosphate as a dispersant to the slurry before sand-milling), and after dilution, the slurry concentration is 200g / L. The pH is 7; polymer chain PVP modified titanium dioxide particles, add 8wt% polymer to the slurry, keep the temperature at room temperature, turn on stirring and ultrasound, turn off the ultrasound after 10 minutes;
[0051] S2 Adjust the pH of the slurry to 2 with dilute acid, adjust it within 15 minutes, and homogenize for 15 minutes. Add 15% aniline monomer to the titanium dioxide slurry, stir and homogenize at room temperature for 6 hours, and then add the initiator ammonium persulfate to the slurry to initiate monomer polymerization. This process requires ultrasonic assistance and lasts for 2 hours. Then after raising the system temperature to 60°C, homogenize for 1...
Embodiment 3
[0054] A preparation method of conductive titanium dioxide, comprising the following steps:
[0055] S1 Uncoated titanium dioxide is pulverized, wet-milled, sand-milled (add 1% sodium hexametaphosphate as a dispersant to the slurry before sand-milling), and after dilution, the slurry concentration is 300g / L. The pH is 7; polymer chain PVP modified titanium dioxide particles, add 8wt% polymer to the slurry, keep the temperature at room temperature, turn on stirring and ultrasound, turn off the ultrasound after 10 minutes;
[0056] S2 Adjust the pH of the slurry to 2 with dilute acid, adjust it within 15 minutes, and homogenize for 15 minutes. Add 15% aniline monomer to the titanium dioxide slurry, stir and homogenize at room temperature for 6 hours, and then add the initiator ammonium persulfate to the slurry to initiate monomer polymerization. This process requires ultrasonic assistance and lasts for 3 hours. Then after raising the system temperature to 60°C, homogenize for 1...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com