Application of tungsten-based solid acid in lactic acid and lactate preparation using biomass and saccharides
A technology of biomass and solid acid, which is applied in the preparation of carboxylate, carboxylate, and organic compounds, etc. It can solve the problems of long preparation period of Sn-β molecular sieve, difficult catalytic conversion of biomass, complex preparation process, etc. , achieving good application prospects, favorable cost, and simple preparation
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0027] (1) Ba-WO 3 Catalyst preparation: Take 0.1mol lithium tungstate and 0.5mol barium chloride into 4L deionized water, add 3mol / L hydrochloric acid to adjust the pH value to 1.5 and stir for 1h; In the synthesis kettle, synthesize at 160°C for 72h, take out the synthesized solid, wash and dry to obtain Ba-WO 3 catalyst.
[0028] (2)Ba-WO 3 Catalytic conversion of biomass sugars by catalyst: take 0.2gBa-WO 3 Catalyst, 4g of fructose, 20ml of methanol, 20ml of methyl lactate were added to the autoclave, and after purging the air with nitrogen, the reaction was carried out at 150°C for 300min to obtain a yield of methyl lactate (relative to the fructose raw material) of 73mol%.
Embodiment 2
[0030] (1) Ca-WO 3 Catalyst preparation: Take 0.5mol sodium tungstate, 0.5mol potassium tungstate and 0.6mol calcium chloride into 4L deionized water, add 3mol / L nitric acid to adjust the pH value to 1 and stir for 3h; In the hydrothermal synthesis kettle of tetrafluoroethylene, synthesize at 240°C for 3h, take out the synthesized solid, wash and dry to obtain Ca-WO 3 catalyst.
[0031] (2) Ca-WO 3 Catalytic conversion of biomass sugars by catalyst: Take 0.1g Ca-WO 3 Catalyst, 5g of glucose, and 40ml of water were added to the autoclave, and after purging the air with nitrogen, the reaction was carried out at 160° C. for 280 minutes to obtain a yield of lactic acid (relative to the glucose raw material) of 88 mol%.
Embodiment 3
[0033] (1) Pb-WO 3 Catalyst preparation: Take 2.4mol potassium tungstate, 0.6mol tungsten chloride and 1.5mol lead nitrate into 4L deionized water, add 3mol / L hydrochloric acid and sulfuric acid with a molar ratio of 1:1 mixed acid to adjust the pH value to 3 and Stir for 3h; transfer the above solution to a hydrothermal synthesis kettle with polytetrafluoroethylene, synthesize at 180°C for 20h, take out the synthesized solid, wash, and dry to obtain Pb-WO 3 catalyst.
[0034] (2)Pb-WO 3 Catalyst for catalytic conversion of biomass sugars: take 0.4gPb-WO 3 Catalyst, 3g of maltose, and 40ml of ethanol were added to the autoclave, and after purging the air with nitrogen, the reaction was carried out at 190° C. for 100 min to obtain a yield of ethyl lactate (relative to the raw material of maltose) of 81 mol%.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com