Multi-color epoxy boat topping paint and preparing method thereof
An epoxy waterline and epoxy resin technology, applied in epoxy resin coatings, biocide-containing paints, antifouling/underwater coatings, etc., can solve the problem of lack of preparation methods, unreasonable selection of raw materials, and poor quality. problems, to achieve the effect of easy promotion and use, high market value and wide applicability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] Weigh 50kg of epoxy resin, 1kg of organic soil, 18kg of precipitated barium sulfate, 6kg of xylene, 1kg of butanol, 1kg of amino resin, 5kg of chlorinated rubber liquid, 2kg of tributyltin fluoride, 3kg of zinc oxide, 4kg of urea, and 2kg of permanent asphalt, 2kg of sodium silicate, 5kg of methyl isobutyl ketone, 8kg of pigment, 2kg of anti-sedimentation agent, and 60kg of deionized water.
[0019] The anti-settling agent is polyethylene wax or hydrogenated castor oil.
[0020] The organic soil is prepared by mixing equal amounts of silicon dioxide, aluminum oxide, iron oxide, calcium oxide, manganese oxide, potassium oxide, silicon dioxide and caustic soda.
[0021] The pigments are all extracted from herbal plants and are non-toxic and harmless.
[0022] The preparation method is as follows:
[0023] (1) Choose a dispersion kettle, add the above epoxy resin, amino resin and modified asphalt, then add deionized water and chlorinated rubber liquid, stir and mix at 20...
Embodiment 2
[0027] Weigh 55g of epoxy resin, 1.5g of organic soil, 20g of precipitated barium sulfate, 6.6g of xylene, 1.5g of butanol, 1.8g of amino resin, 6g of chlorinated rubber liquid, 3g of tributyltin fluoride, 4g of zinc oxide, Urea 5g, modified asphalt 3g, sodium silicate 3g, methyl isobutyl ketone 6g, pigment 9g, anti-settling agent 4g, deionized water 65g.
[0028] The anti-settling agent is polyethylene wax or hydrogenated castor oil.
[0029] The organic soil is prepared by mixing equal amounts of silicon dioxide, aluminum oxide, iron oxide, calcium oxide, manganese oxide, potassium oxide, silicon dioxide and caustic soda.
[0030] The pigments are all extracted from herbal plants and are non-toxic and harmless.
[0031] The preparation method is as follows:
[0032] (1) Choose a dispersion kettle, add the above epoxy resin, amino resin and modified asphalt, then add deionized water and chlorinated rubber liquid, stir and mix at 20-50°C for 20-25 minutes, stir well and then...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com