Aluminium calcium manganese titanium iron alloy for steel-smelting deoxygenation and alloying
A technology of aluminum calcium manganese titanium and iron alloys, applied in the field of iron alloys, can solve the problems of easy condensation, unfavorable continuous casting and high melting point
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment
[0012] Adopt above-mentioned first method, according to containing aluminum 89% aluminum ingot 349Kg, calcium iron 36Kg containing calcium 89%, manganese containing 75% ferromanganese 48Kg, titanium containing 85% ferrotitanium 11Kg and steel scrap 156Kg batching, divide The horse is placed in a power frequency induction furnace, heated and melted, fully melted into a liquid state, released from the furnace, cast ingots, broken into pieces, and the chemical composition (weight %) obtained is: AI57, Ca6, Mn6, Ti1.5, and the balance is Fe and Alcalcium-manganese-titanium-iron alloy with unavoidable impurities.
[0013] Using the above-mentioned alloy instead of ZL98120546.1 patented alloy as a deoxidizer for smelting titanium-containing low-alloy and micro-alloy steel, the contents of [O], [S] and inclusions in the steel are reduced, and the impact toughness and elongation of the steel are improved.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com