Examples
Embodiment 1
[0012] Select foamed nickel metal with a connected porosity of 90-95% VOL (volume percentage) as the carrier, pre-treat and activate the foamed nickel, and then uniformly plate 0.1-2 microns on its surface by electroplating, electroless plating or displacement plating. of silver plating. Then the silver-loaded nickel foam mesh is used for air filtration and purification of air purifiers, central air conditioners, and household air conditioners, which has a very obvious effect, and can effectively kill the germs that are filtered and adsorbed on the foam metal mesh.
Embodiment 2
[0014] The silver-loaded hydroxyapatite nanopowder slurry was prepared by chemical precipitation method. According to Ca9.5Ag0.5 (PO 4 ) 6 (OH) 2 Composition, weigh Ca(NO 3 ) 2 ·6H 2 O 23.6g was dissolved in 400ml distilled water to prepare Ca(NO 3 ) 2 solution. Weigh AgNO 3 0.85g dissolved in the above Ca(NO 3 ) 2 solution, mixed evenly to obtain A solution.
[0015] Take another (NH 4 ) 2 HPO 4 7.92g was dissolved in 200ml of distilled water, 15ml of ammonia water was measured, and dissolved in the above (NH 4 ) 2 HPO 4 solution, after mixing evenly, dilute the solution to 400ml to obtain B solution.
[0016] Add the above B solution drop by drop to the A solution, keep stirring, and control the solution temperature to 30°C. At this time, the solution starts to become turbid, and there is precipitation. After the drop is complete, stop stirring, and keep the solution for 12 hours. . After suction filtration and washing with water several times, the obtai...
Embodiment 3
[0020] The preparation method of the silver-loaded hydroxyapatite nanopowder slurry is the same as in Example 2.
[0021] After the slurry obtained by the above method was dried, it was calcined at 800° C. for 4 hours. The obtained powder is added with 0.5% organic additive as a slurry stabilizer according to the mass ratio, and additionally 30% of nano titanium oxide particles are added to prepare a stable slurry in a planetary ball mill.
[0022] Spray the slurry on the surface of the nickel foam filter and let it dry in a ventilated place. The modified silver-loaded hydroxyapatite sterilization filter can be obtained by drying in an oven at 120° C. for 8 hours.
[0023] The modified silver-loaded hydroxyapatite bactericidal filter is applied to air purification and filtration, and the photocatalytic effect of nano-titanium dioxide is used with ultraviolet light irradiation, which has better ability to kill germs.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com