Stretch-resistant metal casting
A technology of metal casting and stretch resistance, which is applied in the field of metal casting, can solve the problems that need to be further improved, and achieve the effect of enhancing mechanical properties, ensuring stretch resistance, and improving stretch resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] A stretch-resistant metal casting, comprising the following substances in parts by mass: 90 parts of iron, 0.5 part of polonium, 1 part of iridium, 1 part of osmium, 1 part of palladium, 1 part of molybdenum, 1 part of manganese, 1 part of zirconium, and 1 part of yttrium 1 part of silicon, 1 part of copper, 1 part of scandium, 1 part of chromium, 1 part of tellurium, 1 part of nickel, and other unavoidable trace impurities. The smelting sequence is as follows: first smelt scrap steel, send samples for analysis, then put polonium, iridium, osmium, palladium, molybdenum, manganese, zirconium, yttrium, silicon, copper, scandium, chromium, tellurium, nickel into Molten steel; after it is completely dissolved, add slagging agent to make slag, analyze and take samples; if the sample is not in proportion, continue to make slag and take samples until it meets the standard, then increase the power of the intermediate frequency furnace, insert a thermocouple, and measure the temp...
Embodiment 2
[0017] A stretch-resistant metal casting, comprising the following substances in parts by mass: 100 parts of iron, 1 part of polonium, 2 parts of iridium, 1.5 parts of osmium, 1.5 parts of palladium, 5 parts of molybdenum, 3 parts of manganese, 3 parts of zirconium, and 1.5 parts of yttrium 2 parts of silicon, 3 parts of copper, 2.4 parts of scandium, 1.5 parts of chromium, 1.5 parts of tellurium, and 2 parts of nickel; the smelting sequence is as follows: first smelt the scrap steel, send samples for analysis, and mix polonium, iridium, osmium , palladium, molybdenum, manganese, zirconium, yttrium, silicon, copper, scandium, chromium, tellurium, and nickel are baked and then put into molten steel; Slagging and sampling until it meets the standard, then increase the power of the intermediate frequency furnace, insert a thermocouple, measure the temperature of the molten steel at 1600 ° C to reach the outlet temperature, then deoxidize, come out of the furnace, and finally cast ...
Embodiment 3
[0019] A stretch-resistant metal casting, comprising the following substances in parts by mass: 110 parts of iron, 1.5 parts of polonium, 3 parts of iridium, 2 parts of osmium, 2 parts of palladium, 10 parts of molybdenum, 5 parts of manganese, 5 parts of zirconium, and 2 parts of yttrium 3 parts of silicon, 5 parts of copper, 4 parts of scandium, 2 parts of chromium, 2 parts of tellurium, 3 parts of nickel, and other unavoidable trace impurities. The smelting sequence is as follows: first smelt scrap steel, send samples for analysis, then put polonium, iridium, osmium, palladium, molybdenum, manganese, zirconium, yttrium, silicon, copper, scandium, chromium, tellurium, nickel into Molten steel; after it is completely dissolved, add slagging agent to make slag, analyze and take samples; if the sample is not in proportion, continue to make slag and take samples until it meets the standard, then increase the power of the intermediate frequency furnace, insert a thermocouple, and ...
PUM
Property | Measurement | Unit |
---|---|---|
diameter | aaaaa | aaaaa |
length | aaaaa | aaaaa |
tensile strength | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com