Novel high-performance anti-corrosion and waterproofing environment-friendly material
A new material and high-performance technology, applied in the field of anti-corrosion and waterproof materials, can solve problems such as potential safety hazards, and achieve the effects of good heat resistance, simple process operation, and easy availability of raw materials
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] A new high-performance, anti-corrosion, waterproof and environmentally friendly material proposed by the present invention comprises the following raw materials in parts by weight: 28 parts of neoprene rubber, 20 parts of polyvinyl chloride resin, 10 parts of acrylonitrile-butadiene-styrene resin, and 7 parts of zinc oxide , 5 parts of benzoic acid, 10 parts of white carbon black, 5 parts of dibutyl hydroxytoluene, 4 parts of zinc soap, 4 parts of dihydropyridine, 3 parts of light stabilizer, and 8 parts of water-based waterproofing agent.
[0021] Its preparation method comprises the following steps:
[0022] S1. Add the neoprene rubber with the specific gravity into a rubber vulcanization tank, add zinc oxide and benzoic acid with the specific gravity, vulcanize for 5 hours at a high temperature of 165°C, and set aside;
[0023] S2. Add the acrylonitrile-butadiene-styrene resin of the specific gravity into a crucible melting furnace, heat at a high temperature of 245°...
Embodiment 2
[0029] A new high-performance, anti-corrosion, waterproof and environmentally friendly material proposed by the present invention comprises the following raw materials in parts by weight: 30 parts of neoprene rubber, 24 parts of polyvinyl chloride resin, 12 parts of acrylonitrile-butadiene-styrene resin, and 6 parts of zinc oxide , 4 parts of benzoic acid, 11 parts of white carbon black, 6 parts of dibutyl hydroxytoluene, 5 parts of zinc soap, 3 parts of dihydropyridine, 2 parts of light stabilizer, and 10 parts of water-based waterproofing agent.
[0030] Its preparation method comprises the following steps:
[0031] S1. Add the neoprene rubber with the specific gravity into a rubber vulcanization tank, add zinc oxide and benzoic acid with the specific gravity, vulcanize for 7 hours at a high temperature of 155°C, and set aside;
[0032] S2. Add the acrylonitrile-butadiene-styrene resin of the specific gravity into a crucible melting furnace, heat at a high temperature of 250...
Embodiment 3
[0038] A new high-performance, anti-corrosion, waterproof and environmentally friendly material proposed by the present invention comprises the following raw materials in parts by weight: 42 parts of neoprene rubber, 30 parts of polyvinyl chloride resin, 15 parts of acrylonitrile-butadiene-styrene resin, and 10 parts of zinc oxide , 8 parts of benzoic acid, 15 parts of white carbon black, 9 parts of dibutyl hydroxytoluene, 8 parts of zinc soap, 8 parts of dihydropyridine, 7 parts of light stabilizer, and 15 parts of water-based waterproofing agent.
[0039] Its preparation method comprises the following steps:
[0040] S1. Add the neoprene rubber with the specific gravity into a rubber vulcanization tank, add zinc oxide and benzoic acid with the specific gravity, vulcanize at a high temperature of 170°C for 4 hours, and set aside;
[0041] S2. Add the acrylonitrile-butadiene-styrene resin of the specific gravity into a crucible melting furnace, heat at a high temperature of 23...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com